Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
Pyrotek S-679 Dense Graphite Material Treated for Oxidation Resistance S-679 is an isostatically pressed graphite material that is treated to provide oxidation resistance at elevated temperatures. This material performs well in glass contact applications where heat an.. |
|||
Thermal Conductivity | 45.0 W/m-K @Temperature 85.0 °C |
312 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 9 Sn-Pb-In Solder Alloy General purpose solder in 160° C range with good physical properties.Information provided by the manufacturer, Indium Corporation. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
ThyssenKrupp XABO® 355 Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
ThyssenKrupp XABO® 500 T Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
ThyssenKrupp XABO® 355 T Structural Steel This Material Specification applies to thermomechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
ThyssenKrupp XABO® 500 Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
Eagle Brass 706 Copper Nickel 10%, 1/2 Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
Eagle Brass 706 Copper Nickel 10%, 1/4 Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
Eagle Brass 706 Copper Nickel 10%, Annealed 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
Eagle Brass 706 Copper Nickel 10%, Extra Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
Eagle Brass 706 Copper Nickel 10%, Hard 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
Eagle Brass 706 Copper Nickel 10%, Spring 706 exhibits excellent corrosion resistance, especially in marine applications. It has a relatively high strength and has resistance at elevated temperatures. The cost is relatively high compared to.. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
ThyssenKrupp XABO® 460 Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |
|||
Thermal Conductivity | 45.0 W/m-K | 312 BTU-in/hr-ft²-°F | |
ThyssenKrupp XABO® 460 T Structural Steel This Material Specification applies to thermo mechanically rolled flat products in thicknesses up to 60 mm. The criteria to distinguish the steel grades is the lowest test temperature for the notch-.. |