Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 41.8 W/m-K @Temperature 10.0 - 232 °C |
290 BTU-in/hr-ft²-°F @Temperature 50.0 - 450 °F |
|
Meehanite GE-30 Flake Graphite Cast Iron Type GE-30 combines improved strength and solidity with higher machining feeds and speeds than ordinary gray iron.General Meehanite information - Meehanite metal is first melted to a definite degree.. |
|||
Thermal Conductivity | 41.8 W/m-K | 290 BTU-in/hr-ft²-°F | |
Atom Adhesives AA-DUCT AD1 Epoxy Adhesive AA-DUCT AD1 is a single component epoxy, formulated with pure silver power combined with organic binders and solvents to produce electrically conductive paths, films or patterns over non-conductive .. |