Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Thermal Conductivity = 36.0 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 36.0 W/m-K
250 BTU-in/hr-ft²-°F
McDanel Advanced Ceramics 99.8% Alumina
Information provided by McDanel Advanced Ceramic Technologies
Thermal Conductivity 36.0 W/m-K

@Temperature 85.0 °C
250 BTU-in/hr-ft²-°F

@Temperature 185 °F
Indium Corp. Indalloy® 8 In-Sn-Cd Fusible Alloy
General purpose fusible alloy.Information provided by the manufacturer, Indium Corporation.
Thermal Conductivity 36.0 W/m-K
250 BTU-in/hr-ft²-°F
Williams Advanced Alloys WS302 Solder
All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys
Thermal Conductivity 36.0 W/m-K
250 BTU-in/hr-ft²-°F
Eagle Brass 1008 Low Carbon Steel, 1/4 Hardened
1008 is a standard grade Carbon Steel. This alloy is generally used for "commercial quality" cold rolled steel. It is an economical, general purpose steel grade offering moderate strength and toughn..
Thermal Conductivity 36.0 W/m-K
250 BTU-in/hr-ft²-°F
Eagle Brass 1008 Low Carbon Steel, Full Hardened
1008 is a standard grade Carbon Steel. This alloy is generally used for "commercial quality" cold rolled steel. It is an economical, general purpose steel grade offering moderate strength and toughn..
Thermal Conductivity 36.0 W/m-K
250 BTU-in/hr-ft²-°F
Eagle Brass 1008 Low Carbon Steel, 1/2 Hardened
1008 is a standard grade Carbon Steel. This alloy is generally used for "commercial quality" cold rolled steel. It is an economical, general purpose steel grade offering moderate strength and toughn..
Thermal Conductivity 36.0 W/m-K
250 BTU-in/hr-ft²-°F
Eagle Brass 1008 Low Carbon Steel, Annealed
1008 is a standard grade Carbon Steel. This alloy is generally used for "commercial quality" cold rolled steel. It is an economical, general purpose steel grade offering moderate strength and toughn..
Thermal Conductivity 36.0 W/m-K
250 BTU-in/hr-ft²-°F
Aremco Ceramacast™ 673 Castable Ceramic
Chemical setting. Two-part ceramic exhibiting high thermal conductivity. Used to pot small temperature sensors, gas igniters, and high intensity lights. Applied in areas up to 1" diameter by 1" de..
Copyright © lookpolymers.com All Rights Reserved