Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 359.7 W/m-K | 2496 BTU-in/hr-ft²-°F | |
Eagle Brass 151 ZHC® COPPER, 1/2 Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Thermal Conductivity | 359.7 W/m-K | 2496 BTU-in/hr-ft²-°F | |
Eagle Brass 151 ZHC® COPPER, 1/4 Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Thermal Conductivity | 359.7 W/m-K | 2496 BTU-in/hr-ft²-°F | |
Eagle Brass 151 ZHC® COPPER, 3/4 Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Thermal Conductivity | 359.7 W/m-K | 2496 BTU-in/hr-ft²-°F | |
Eagle Brass 151 ZHC® COPPER, Annealed Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Thermal Conductivity | 359.7 W/m-K | 2496 BTU-in/hr-ft²-°F | |
Eagle Brass 151 ZHC® COPPER, Extra Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Thermal Conductivity | 359.7 W/m-K | 2496 BTU-in/hr-ft²-°F | |
Eagle Brass 151 ZHC® COPPER, Hard Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Thermal Conductivity | 359.7 W/m-K | 2496 BTU-in/hr-ft²-°F | |
Eagle Brass 151 ZHC® COPPER, Spring Alloy C151 has excellent solderability, high conductivity, and good strength. C151 has superior high temperature softening resistance compared to pure copper C110.Applications can be found in high c.. |
|||
Thermal Conductivity | 359.7 W/m-K | 2496 BTU-in/hr-ft²-°F | |
Cadi 162 Copper Alloy Cadmium addition to copper increases hardness and resistance to softening. C16200 is utilized in numerous applications where fatigue strength and high electrical conductivity are required. Cadmium.. |