Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-160® alloy plate, aged 1000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-160® alloy plate, aged 4000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-160® alloy, annealed plate Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-160® alloy, plate, aged 1000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-160® alloy, plate, aged 1000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-160® alloy, plate, aged 4000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-160® alloy, plate, aged 8000 hours at 760°C (1400°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-160® alloy, plate, aged 8000 hours at 871°C (1600°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 26.1 W/m-K @Temperature 800 °C |
181 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-160® alloy plate, aged 8000 hours at 649°C (1200°F) Outstanding resistance to various forms of high-temperature corrosion attack, excellent resistance to sulfidation and chloride attack in both reducing and oxidizing atmospheres. Excellent forming an.. |
|||
Thermal Conductivity | 26.1 W/m-K | 181 BTU-in/hr-ft²-°F | |
Eagle Brass 430 Ferritic Stainless Steel, 1/2 Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
Thermal Conductivity | 26.1 W/m-K | 181 BTU-in/hr-ft²-°F | |
Eagle Brass 430 Ferritic Stainless Steel, 1/4 Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
Thermal Conductivity | 26.1 W/m-K | 181 BTU-in/hr-ft²-°F | |
Eagle Brass 430 Ferritic Stainless Steel, Annealed Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |
|||
Thermal Conductivity | 26.1 W/m-K | 181 BTU-in/hr-ft²-°F | |
Eagle Brass 430 Ferritic Stainless Steel, Full Hardened Type 430 is one of the most widely used of the "non-hardenable" ferritic stainless steels. It combines good corrosion resistance and heat and oxidation with good mechanical properties. Typical pro.. |