Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | |
Misumi DC53 JIS Tool Steel General purpose cold work die and mold steel whose strength and toughness approach those of high speed steels. Good machinability and grindability. Tougher than D2 Tool Steel. Machines 30% faster th.. |
|||
Thermal Conductivity | 23.8 W/m-K @Temperature 800 °C |
165 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-120® alloy, solution heat-treated Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 23.8 W/m-K @Temperature 800 °C |
165 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1200°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 23.8 W/m-K @Temperature 800 °C |
165 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1400°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 23.8 W/m-K @Temperature 800 °C |
165 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1600°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 23.8 W/m-K @Temperature 800 °C |
165 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes HR-120® alloy, solution heat-treated aged at 1800°F for 1000 hours Excellent strength at elevated temperatures, combined with good resistance to carburizing and sulfidizing environments. Applications include bar frame heat treating baskets, wire mesh furnace belts .. |
|||
Thermal Conductivity | 23.8 W/m-K @Temperature 800 °C |
165 BTU-in/hr-ft²-°F @Temperature 1470 °F |
|
Haynes 718 alloy, cold rolled, solution-treated and aged sheet Cb and Ta content combined weight percentage of 5. Excellent high-temperature strength up to 650°C, good ductility, formability, and weldability. Very good welding characteristics. Applications i.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed and Aged Rod and Bar specifically. Other property values are typic.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Annealed and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 or.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed and Aged Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed and Aged Wire specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy i.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | Age Hardened |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Annealed Rod and Bar specifically. Other property values are typical of ann.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | Age Hardened |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Strip Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Annealed Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 3.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | Age Hardened |
Special Metals DURANICKEL® 301 (UNS N03301) Annealed Wire Tensile strength (ultimate) and elongation values reported here are typical for Annealed Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gen.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn and Aged Rod and Bar Tensile strength (ultimate and yield), compressive strength, hardness, and elongation values reported here are typical for Cold-Drawn and Aged Rod and Bar specifically. Other property values are typ.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | Age Hardened |
Special Metals DURANICKEL® 301 (UNS N03301) Cold-Drawn Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Cold-Drawn Rod and Bar specifically. Other property values are typical of annealed DURANICKEL®.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | |
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard and Aged Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard and Aged Strip specifically. Other property values are typical of aged DURANICKEL® alloy 301 o.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | Age Hardened |
Special Metals DURANICKEL® 301 (UNS N03301) Half-Hard Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Half-Hard Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished and Aged Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished and Aged Rod and Bar specifically. Other property values are typical of aged DURANIC.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | Age Hardened |
Special Metals DURANICKEL® 301 (UNS N03301) Hot-Finished Rod and Bar Tensile strength (ultimate and yield), hardness, and elongation values reported here are typical for Hot-Finished Rod and Bar specifically. Other property values are typical of annealed DURANICKELÂ.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | Age Hardened |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the al.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Strip, Aged Tensile strength (ultimate), hardness, and elongation values reported here are typical for Spring Strip, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the .. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | Age Hardened |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire specifically. Other property values are typical of annealed DURANICKEL® alloy 301 or the alloy in gener.. |
|||
Thermal Conductivity | 23.8 W/m-K | 165 BTU-in/hr-ft²-°F | |
Special Metals DURANICKEL® 301 (UNS N03301) Spring Wire, Aged Tensile strength (ultimate) and elongation values reported here are typical for Spring Wire, Aged specifically. Other property values are typical of aged DURANICKEL® alloy 301 or the alloy in gen.. |