Polymer Property : Thermal Conductivity = 221.3 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 221.3 W/m-K
1536 BTU-in/hr-ft²-°F
Materion Alloy 390 Beryllium Nickel Strip
Alloy 390 was specifically designed for high power applications, providing a unique combination of high strength and high conductivity. Increasing power requirements are driving the need for lower c..