Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 210 W/m-K @Temperature 20.0 - 400 °C |
1460 BTU-in/hr-ft²-°F @Temperature 68.0 - 752 °F |
|
Hogen Duralloy H3W 68 Tungsten/32 Copper PM Metal Composite RWMA Class 10.Hogen Duralloy refractory alloys are manufactured by pressing, sintering, and infiltrating tungsten with copper or silver.Typical Resistance Welding Applications: Class 10 material is .. |
|||
Thermal Conductivity | 210 - 220 W/m-K | 1460 - 1530 BTU-in/hr-ft²-°F | x-y direction |
MarkeTech Cu/Mo/Cu 1:4:1 Laminated Sheet Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea.. |
|||
Thermal Conductivity | 210 - 220 W/m-K | 1460 - 1530 BTU-in/hr-ft²-°F | x-y direction |
MarkeTech Cu/Mo70-Cu30/Cu 1:4:1 Laminated Sheet Cu/Mo/Cu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated he.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915â„¢ Annealed Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915â„¢ Hard Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | Typical |
Materion E20 Beryllium/BeO Composite, 20 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | Through Thickness |
GrafTech M3 Thin Aluminum Foil Coating Optional coating for eGRAF® SPREADERSHIELD™ graphite products. Structure: 0.127mm Al - 0.025mm PSA |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion AlBeMet® AM 162 HIP'd Billet, Annealed This is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are derived by consolidating the Al/Be powder by hot isostatic pressing (HIP) .. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915â„¢ Annealed Temper Wire Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915™ AT Temper Rod Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915™ AT Temper Wire Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915â„¢ Hard Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: as suppliedBrush 1915â„¢ is Brush Wellman's new heat-treatable leaded copper alloy. Engineered spe.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915™ Heat Treated Temper Rod, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°C or Mill HardenedBrush 1915™ is Brush Wellman's new heat-treatable leaded coppe.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.050" - 0.375" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion Brush 1915™ Heat Treated Temper Wire, 0.375" - 0.500" Information supplied by Brush Wellman Engineered Materials.Treatment required for max strength: 3.5 hrs @ 370°CBrush 1915™ is Brush Wellman's new heat-treatable leaded copper alloy. Enginee.. |
|||
Thermal Conductivity | >= 210 W/m-K | >= 1460 BTU-in/hr-ft²-°F | Minimum |
Materion E60 Beryllium/BeO Composite, 60 Volume% BeO Metal matrix composite made up principally of beryllium and crystal BeO platelets. Produced by blending the beryllium and beryllium oxide powders into a homogeneous mixture to create isotropic prop.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | ASTM E1461 |
M Cubed Technologies TSC-15 Titanium-alloyed Reaction Bonded Silicon Carbide Specialty reaction-bonded SiC for applications requiring high stiffness, high toughness, and also high thermal conductivity--mechanical seals, for example Flow-through complex channels can be forme.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Ametek Molybdenum-Copper Composite AMC 6436 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion AlBeMet® AM 162 Extruded Bar, Annealed Mechanical property values below are in the longitudinal direction; transverse values generally lower. This is a powder metallurgical product produced by gas atomization available as rod, bar, tube.. |
|||
Thermal Conductivity | 210 W/m-K | 1460 BTU-in/hr-ft²-°F | |
Materion AlBeMet® AM 162 Rolled Sheet, Annealed Mechanical properties are typical, longitudinal values at RT. AlBeMet® AM 162 is a powder metallurgical product produced by gas atomization available as rod, bar, tube and sheet. These shapes are.. |