Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 175 W/m-K | 1210 BTU-in/hr-ft²-°F | Estimated by Poco |
Poco Graphite AXF-5QC Specialty Graphite, Copper Impregnated SSH hardness is 67.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p.. |
|||
Thermal Conductivity | 175 W/m-K | 1210 BTU-in/hr-ft²-°F | |
Poco Graphite DFP-1C (Copper impregnated) Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
Thermal Conductivity | 175 W/m-K | 1210 BTU-in/hr-ft²-°F | |
PCC-Advanced Forming Technology 63% AlSiC Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
Thermal Conductivity | 175 W/m-K | 1210 BTU-in/hr-ft²-°F | |
PCC-Advanced Forming Technology 68% AlSiC Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
Thermal Conductivity | 175 W/m-K | 1210 BTU-in/hr-ft²-°F | |
PCC-Advanced Forming Technology 70% AlSiC Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
Thermal Conductivity | 175 W/m-K | 1210 BTU-in/hr-ft²-°F | |
PCC-Advanced Forming Technology AlSiC-SD Metal Matrix Composite AlSiC metal matrix composites are formed by pressure infiltrating molten aluminum into silicon carbide preforms. This method of casting is typically used in applications where solution requirements .. |
|||
Thermal Conductivity | 175 W/m-K | 1210 BTU-in/hr-ft²-°F | |
CMW® ELKONITE® 3150 Silver Tungsten Carbide contact material ASTM B663 Table 2, Class B For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc. |
|||
Thermal Conductivity | 175 W/m-K | 1210 BTU-in/hr-ft²-°F | |
CMW® ELKONITE® G13 Tungsten Carbide Silver contact material ASTM 663, Class B, infiltrated For arcing and current carrying electrical contacts resistant to welding and sticking.Information provided by CMW Inc. |
|||
Thermal Conductivity | 175 W/m-K | 1210 BTU-in/hr-ft²-°F | |
Ametek Molybdenum-Copper Composite AMC 8020 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |
|||
Thermal Conductivity | 175 W/m-K | 1210 BTU-in/hr-ft²-°F | |
Ametek Tungsten-Copper Composites AWC 9010 Information supplied by Ametek Specialty Metal Products.The material is available as finished parts with the following maximum dimensions:Width: 6 inches (152 mm)Thickness: 0.150 inches (3.8 mm)Leng.. |