Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 0% cold reduction Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 10% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 30% cold reduction Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 30% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 30% cold reduction, 1065°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 40% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 50% cold reduction, 1121°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, all-weld metal GTAW Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, bar after 16000 hours at 648°C Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, bar, after 1000 hours at 650°C (1200°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, bar, after 1000 hours at 870°C (1600°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, bar, after 4000 hours at 650°C (1200°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, bar, after 4000 hours at 760°C (1400°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, bar, after 8000 hours at 650°C (1200°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, bar, after 8000 hours at 870°C (1600°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, sheet after 1000 hours at 648°C Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, sheet after 1000 hours at 760°C (1400°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K | 120 BTU-in/hr-ft²-°F | |
SGL Carbon Group EK 2230 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Thermal Conductivity | 17.3 W/m-K | 120 BTU-in/hr-ft²-°F | |
SGL Carbon Group EK 2240 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Thermal Conductivity | 17.3 W/m-K | 120 BTU-in/hr-ft²-°F | |
SGL Carbon Group EK 2243 Carbon Graphite Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 65.0 °C |
120 BTU-in/hr-ft²-°F @Temperature 149 °F |
|
Crucible Steel CPM® S90V® (420V®) Tool Steel CPM S90V is a unique tool steel made by the Crucible Particle Metallurgy process. It is a martensitic stainless steel with a high volume of vanadium carbides for exceptionally good wear resistance. .. |
|||
Thermal Conductivity | 17.3 W/m-K | 120 BTU-in/hr-ft²-°F | |
Carpenter Kovar® Alloy (Glass and Ceramic Sealing Alloy) Data provided by Carpenter Technology Corporation.Kovar® alloy is a vacuum melted, Fe-Ni-Co, low expansion alloy whose chemical composition is controlled within narrow limits to assure precise unif.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 20% cold reduction Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 20% cold reduction, 1010°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 20% cold reduction, 1065°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 30% cold reduction, 1121°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 40% cold reduction Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 50% cold reduction, 1065°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, sheet after 1000 hours at 871°C (1600°F) Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |
|||
Thermal Conductivity | 17.3 W/m-K @Temperature 300 °C |
120 BTU-in/hr-ft²-°F @Temperature 572 °F |
|
Haynes 556® alloy, 40% cold reduction, 1065°C anneal for 5 minutes Effective resistance to sulfidizing, carburizing, and chlorine-bearing environments at high temperature; good oxidation resistance, fabricability, and excellent high-temperature strength; resists co.. |