Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 17.0 W/m-K @Temperature 200 °C |
118 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Outokumpu 2205 Duplex Stainless Steel Duplex stainless combining high mechanical strength with good corrosion resistance.Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical t.. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 200 °C |
118 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Outokumpu SAF 2304® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 200 °C |
118 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Outokumpu SAF 2507® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 85.0 °C |
118 BTU-in/hr-ft²-°F @Temperature 185 °F |
|
Indium Corp. Indalloy® 150 Pb-In Solder Alloy Indalloy's #7, #10, #150, #204, #205 and #206 comprise a group of lead-indium solders designed to cover the temperature range of 165°C-275°C. All have the minimum gold-leaching characteristics.. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 20.0 °C |
118 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel URANUS® 35N 23.04 Duplex Stainless Steel with PREN = 24 Description: URANUS® 35N (UR 35N) is a 23% Cr, 4% Nickel, Mo free duplex stainless steel (23.04). The alloy UR 35N has similar corrosion resistance properties similar to 316L. Furthermore, its me.. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 20.0 °C |
118 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel URANUS® 52N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: URANUS® 52N+ (UR 52N+) is a super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to re.. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 20.0 °C |
118 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel URANUS® B6 Multipurpose Austenitic Stainless Steel with PREN = 34 Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t.. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 20.0 °C |
118 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel URANUS® B6 N Multipurpose Austenitic Stainless Steel with PREN = 36 Description: URANUS® B6 (904L) is a multipurpose 20 Cr - 4.3 Mo high corrosion resistance austenitic stainless steel developed 40 years ago by CLI. The UR B6N is alloyed with nitrogen (~ 0.13%) t.. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 20.0 °C |
118 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel URANUS® 47N+ 25 Cr Super Duplex Stainless Steel with PREN = 40 Description: CLI - SAF 2507® is a 25.07 super duplex stainless steel with 25% Cr and a PREN value higher than 40. The minimum guaranteed yield strength is 550 MPa which allows the designer to red.. |
|||
Thermal Conductivity | 17.0 W/m-K | 118 BTU-in/hr-ft²-°F | DIN EN 821-2 |
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2 DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications. |
|||
Thermal Conductivity | 17.0 W/m-K | 118 BTU-in/hr-ft²-°F | |
Williams Advanced Alloys WS280A Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
Thermal Conductivity | 17.0 W/m-K | 118 BTU-in/hr-ft²-°F | |
Bohler-Uddeholm BÖHLER S390 MICROCLEAN® High Speed Steel Description: High speed steel produced by powder-metallurgy methods with highest red hardness, compressive strength and wear resistance. The PM technology imparts to the material also excellent toug.. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 23.0 - 100 °C |
118 BTU-in/hr-ft²-°F @Temperature 73.4 - 212 °F |
|
ATI Allegheny Ludlum AL 2003™ Duplex Stainless Steel Characteristics: superior stress corrosion cracking resistance to Types 316 and 317, yield strength double that of conventional austenitic stainless steel, good corrosion resistance, good chloride s.. |
|||
Thermal Conductivity | 17.0 W/m-K | 118 BTU-in/hr-ft²-°F | |
China-Yixing Longly Refractories 75 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 20.0 °C |
118 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel URANUS® 45N 22Cr 3Mo Duplex Stainless Steel with PREN = 33 or 34 Description: URANUS® 45N (UR 45N) is a nitrogen alloyed (= 0.15%) austenitic-ferritic stainless steel (22.05 type) with improved structure stability and high general, localized and stress corrosion.. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 400 °C |
118 BTU-in/hr-ft²-°F @Temperature 752 °F |
|
Outokumpu 725LN Austenitic Stainless Steel Applications: Wet corrosion resistance and general service.Available in hot rolled plate (Quarto) form. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 200 °C |
118 BTU-in/hr-ft²-°F @Temperature 392 °F |
|
Outokumpu LDX 2101® Duplex Stainless Steel Applications: Pulp and paper industryDesalination plantsFlue-gas cleaningCargo tanks and pipe systems in chemical tankersSeawater systemsFirewalls and blast walls on offshore platformsBridgesCompone.. |
|||
Thermal Conductivity | 17.0 W/m-K @Temperature 20.0 °C |
118 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Industeel URANUS® 45N+ 22% Cr Austenitic-Ferritic Duplex Stainless Steel Description: URANUS® 45N+ (UR 45N+) is a nitrogen alloyed austenitic-ferritic Duplex stainless steel (22.05), with a minimum PREN value guaranteed of 36 due to over-alloying in Molybdenum and Chrom.. |