Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 12.22 W/m-K

@Temperature 23.0 °C
84.81 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 20% Cold Work
Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®..
Thermal Conductivity 12.22 W/m-K

@Temperature 23.0 °C
84.81 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 10% Cold Work
Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®..
Thermal Conductivity 12.22 W/m-K

@Temperature 23.0 °C
84.81 BTU-in/hr-ft²-°F

@Temperature 73.4 °F
Carpenter Gall-Tough® Stainless, Annealed and Cold Drawn Bar, 0% Cold Work
Data provided by Carpenter Technology Corporation.Threshold Galling Stress 103 MPa (higher stress tests not performed). The avg. total volume loss on the wear test is 5 mm³ at 100 rpm.Gall-Tough®..