Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 1.35 W/m-K @Temperature 538 °C |
9.37 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Pyrotek Pyrethrum FA 800 Woven Stainless Steel Fabric Pyrotherm FA 800 is a durable, heat-resistant woven fabric made from 316L stainless steel fibers. The fabric maintains its mechanical strength and cloth-like softness in high temperature, abrasive .. |
|||
Thermal Conductivity | 1.35 W/m-K | 9.37 BTU-in/hr-ft²-°F | |
Mateck Fused Silica IR Grade (SiO2) Optical crystals |
|||
Thermal Conductivity | 1.35 W/m-K @Temperature 20.0 °C |
9.37 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
|
Mateck Fused Silica UV-VIS Grade (SiO2) Optical crystals |
|||
Thermal Conductivity | 1.35 W/m-K | 9.37 BTU-in/hr-ft²-°F | |
UBE Tyranno Grade LoxM Ceramic High Temperature Fiber Description: Tyranno Fiber is the continuous ceramic fiber consisting of Si, Ti or Zr,C and O. Advanced composites reinforced by the Tyranno Fiber are expected to play a very important role in the e.. |
|||
Thermal Conductivity | 1.35 W/m-K | 9.37 BTU-in/hr-ft²-°F | Product Property; ASTM E 1530 |
Arlon Thermabond® T20 (99710W008) 0.008" (0.203 mm) Uncured Silicone Rubber with PTFE Coated Fiberglass Carrier Description: 8 mil thick Thermabond® T20 electrically insulating electronic adhesive.Design/Construction: Liner: FEP Product: Uncured Silicone Rubber Carrier: PTFE Coated FiberglassRecommended Prim.. |