Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.673 W/m-K
4.67 BTU-in/hr-ft²-°F
Schott SF6 Glass
Information Provided by SCHOTT North America, Inc.
Thermal Conductivity 0.673 W/m-K
4.67 BTU-in/hr-ft²-°F
Schott SF6HT Glass
Information Provided by SCHOTT North America, Inc.