Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM C518 |
Rogers Corporation Syron™ 7000 Thermoplastic Circuit Material SYRON™ 7000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. SYRON 7000 is thermally stable, with a .. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM C518 |
Rogers Corporation XT/duroid™ 8000 Thermoplastic Laminate, Circuit Material XT/duroid™ 8000 thermoplastic circuit materials provide an excellent solution for printed circuit board applications used in demanding environmental conditions. XT/duroid 8000 circuit materials ar.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM E1461 |
Park Electrochemical Nelco® N4000-13 EP™ BC® Buried Capacitance™, High-Speed Multifunctional Epoxy Laminate and Prepreg Nelco N4000-13 EP™ is an enhanced epoxy resin system engineered for today’s leadfree requirements where multiple solder reflow at temperatures approaching 260ºC are required. N4000-13 EP provides.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM E1461 |
Park Electrochemical Nelco® N4350-13 RF Microwave Performance, Modified Epoxy The Nelco N4350-13 RF and N4380-13 RF series are enhanced epoxy resin systems specifically engineered to provide a unique solution for design applications that demand outstanding thermal properties,.. |
|||
Thermal Conductivity | 0.350 W/m-K @Temperature 23.0 °C |
2.43 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Along flow; ISO/CD 22007-4 |
Victrex® PEEK 150GL15 Polyetheretherketone, 15% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 15% glass fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding, very easy flow, FDA food conta.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 450GL20 Polyetheretherketone, 20% Glass Fibre Reinforced Product Description:High performance thermoplastic material, 20% carbon fibre reinforced Polyetheretherketone (PEEK), semi crystalline, granules for injection moulding and extrusion, standard flow, .. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 450GL30 30% Glass Fiber Reinforced Product Description: High performance thermoplastic material, 30% glass fibre reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, standard flow, F.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® ST™ ST45GL30 Polyetherketoneetherketoneketone (PEKEKK), 30% Glass Fiber Reinforced Product Description:High performance thermoplastic material, 30% glass fibre reinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, granules for injection moulding, standard flow, c.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52 612 |
3M Dyneon™ TFM™ 1605 Modified PTFE Powder
(discontinued **) Type III, gr. 2 PTFE. Second-generation PTFE that is a chemically modified to allow new designs and processing methods. Very good free-flowing powder properties.Data provided by Dyneon. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52 612 |
3M Dyneon™ 1502 PTFE Powder
(discontinued **) Type VI PTFE. The unique properties of polytetrafluoroethylene (PTFE) makes it an indispensable material for modern industry. PTFE offers the following exceptional characteristics:Inert to a wide r.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Average value: 0.350 W/m-K Grade Count:3 |
Overview of materials for Nylon 66, 10% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 10% Mineral Filled". Specific grades with primary filler content between 5% and 14% are includ.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 19/CF/30 Polyamide 46, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Reduced moment of inertia comp.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 19-7416 Polyamide 46, with carbon fiber and PTFE Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 46/CF/15 Polyamide 46, with carbon fiber, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Strong, stiff parts.Reduced moment of inertia compared with metal parts.Electrically conductive.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM D177 |
Manifattura Cattaneo VESPEL® SP1 Polyimide Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Fluorseals PTFE 25% glass filled Improved compressive strength and wear resistance.Information provided by TEKU GmbH Fluorkunststoffe, a distributor of Fluorseals materials. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105/GF/20/EM/RD PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1105-0706 PEEK, with glass fiber Applications: Automotive industry, textile machinery, medical- and precision engineering, aircraft industry.Strong, stiff parts; impact resistance.Dynamic stressed parts at high movement velocity.Ch.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM C177 |
Unitika UNILATE® 1 SC PET Antistatic gradeUNILATE® products are plate materials prepared by using a polyethylene terephthalate (PET resin) as the main component, blending it with glass staple fiber, inorganic filler, and ot.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | |
Hippe PI Wide temperature range for use. High oxidation resistance. UV stability, low coefficient of linear expansion, good strength at high temperatures, resistance against stress cracking.Information pro.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 406 PTFE, 15% PEEK Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 433 PTFE, 10% Ekonol® Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3ZG6 30% Glass Filled PA6 (Conditioned) Ultramid B3ZG6 is an impact-modified, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3ZG6 BK 30564 30% Glass Filled PA6-1 (Conditioned) Description: Impact-modified and 30% glass fiber reinforced injection-molding grade for technical articles of very high stiffness and toughness, for instance, for vehicle airbag housings and suitcas.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3ZG6 BK30564 30% Glass Filled PA6 (Dry) Ultramid B3ZG6 BK30564 is an impact-modified, pigmented black, 30% glass fiber reinforced injection molding PA6 grade for industrial items having very high impact strength and rigidity. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® A3EG6 30% Glass Filled PA66 (Dry) Ultramid A3EG6 is a 30% glass fiber reinforced injection molding PA66 grade for machinery components and housings of high stiffness and dimensional stability. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | ASTM E1530 |
Solvay Specialty Polymers AvaSpire® AV-621 CF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-621 CF30 is a 30% carbon fiber reinforced version of AvaSpire AV-621. It offers better dimensional stability and warp resistance than 30% carbon fiber reinforced PEEK. The AV-621 CF30 gr.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3WG5 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® B3WG5 BK 00564 25% Glass Filled PA6 (Conditioned) Description: 25% glass-fiber reinforced and heat aging resistant injection-molding grade, for instance, for fan impeller glass-fiber reinforced injection-molding grade for industrial articles and el.. |
|||
Thermal Conductivity | 0.350 W/m-K | 2.43 BTU-in/hr-ft²-°F | Along flow; ISO 22007-4 |
Victrex® PEEK 650GL30 30% Glass Fiber Filled, PolyEtherEtherKetone High performance thermoplastic material, 30% glass fiber reinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection molding and extrusion, low flow, color natural/beige.Typical.. |