Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 101 PC (Asia Pacific) Nonhalogenated, 7.0 MFR, for thicker sections without sinks. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertalon® 6 PLA PA 6, cast (ISO Data) Unmodified cast nylon 6 grade exhibiting characteristics which come very close to those of Ertalon 66 SA. It combines high strength, stiffness and hardness with good creep and wear resistance, heat .. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Quadrant EPP Ertalyte® TX PET + solid lubricant, extruded (ISO Data) Ertalyte TX is a polyethylene terephthalate compound incorporating a uniformly dispersed solid lubricant. Its specific formulation makes it a premium internally lubricated bearing-grade. Ertalyte TX.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 201 PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 201R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. Internal mold release. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 203R PC 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 203R PC (Asia Pacific) 7.0 MFR, for thicker sections without sinks. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® LUX2614 PC (Asia Pacific) 7.0 MFR. Improved flame retardance. UV stabilized for outdoor and lighting. Internal mold release. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E1530 |
Solvay Specialty Polymers AvaSpire® AV-848 GF30 Polyaryletherketone (PAEK)
(Unverified Data**) AvaSpire AV-848 GF30 is a 30% glass fiber-reinforced, high-temperature, polyaryletherketone (PAEK) that has been specifically formulated to provide several performance advantages over comparable gra.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | Through Plane; ASTM E1461 |
Victrex® APTIV® 1000-050 Polyetheretherketone (PEEK) Polymer Film, Semi-Crystalline APTIV PEEK 1000 series films are the unfilled semi-crystalline films made from VICTREX® PEEK polymer. The film provides a material solution for engineers in ultra-high performance applications.APTI.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 23.0 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Average; ISO/CD 22007-4 |
Victrex® PEEK 150G / 151G Polyetheretherketone, Unreinforced Product Description:High performance thermoplastic material, unreinforced Polyetheretherketone (PEEK), semi crystalline, depth filtered granules for injection moulding, easy flow, FDA food contact c.. |
|||
Thermal Conductivity | 0.290 W/m-K @Temperature 23.0 °C |
2.01 BTU-in/hr-ft²-°F @Temperature 73.4 °F |
Average; ISO 22007-4 |
Victrex® ST™ STG45 PolyEtherKetoneEtherKetoneKetone, Unreinforced Product Description:High performance thermoplastic material, unreinforced PolyEtherKetoneEtherKetoneKetone (PEKEKK), semi crystalline, depth filtered granules for injection moulding, standard flow, .. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics PET Polyethylene Terephthalate Polyethylene terephthalate shows high tensile and mechanical strength, hardness and toughness, low friction and a high dimensional stability. PET may be used at temperatures ranging from -20°C to.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8301:1991 |
Global EPP PET PET is an unreinforced, semi-crystalline thermoplastic polyester, demonstrating dimensional stability similar to acetal, combined with the comparable wear resistance of nylon. Heavily loaded mechani.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Haysite H254 Polyester Laminate Solder Pallet and Work Holder Sheet A Static dissipative sheet material for use in electronic assembly. Resistant to hot solder and solvents. Standard color is blue/grey. Available thicknesses from.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL V03550 PPE+HIPS (Asia Pacific) Noryl* V03550 is a 35% milled fibre reinforced, injection moldable grade. Designed for good dimensional stability and low warpage, this resin also uses non-chlorinated, non-brominated FR additives t.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | DIN 52612 |
Schwartz Technical Plastics LAMINEX® 2000 Cotton Fabric, Phenolic Resin Impregnated, Coarse Application: rollneck-bearings, coverts for friction rollsInformation provided by Schwartz Technical Plastics GmbH |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics LNP Lubricomp UX06442 PPA LNP* Lubricomp* UX06442 is a compound based on Polyphthalamide resin containing Proprietary Lubricant. Added features of this material include: Internally Lubricated.This data was supplied by SABIC.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM AR9300 PEI (Europe-Africa-Middle East) 30% Glass fiber filled, standard flow Polyetherimide (Tg 217C). Meets FAR 25.853 and OSU 65/65 with low toxicity, smoke, and flame evolution. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers Ryton® QA200P Polyphenylene Sulfide (PPS) Ryton® QA200P (pelletized) unfilled polyphenylene sulfide exhibits excellent thermal stability and chemical resistance and may be used in injection molding processes.Features: Good Chemical Resis.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Trelleborg Emerson & Cuming Stycast® XT-1122 Two-Component Epoxy Flexible Encapsulant Emerson & Cuming XT-1122 Stycast® Two-Component Epoxy Flexible EncapsulantHeat, thermal shock and impact resistance. Good chemical resistance, Low Viscosity, Unfilled. Mix Ratio (by weight) = 100:6.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Dow CYCLOTENE™ 3022-35 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Dow CYCLOTENE™ 3022-46 Bisbenzocyclobutene (BCB) Electronic Resin This product was developed for use as spin-on dieletric materials in microelectronic fabrication.Information provided by Dow |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Dow CYCLOTENE™ 4024-40 Advanced Electronic Resins (PhotoBisbenzocyclobutene BCB) CYCLOTENE™ 4024-40 advanced electronic resin is I-line-, G-line-, and broad band-sensitive photopolymer that has been developed for use as a dielectric in thin film microelectronic applications.Inf.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ISO 8302 |
Eurostar Staramide B28H PA6, Heat Stabilized, Injection Molded Staramide B28H is a Heat Stabilized, Unreinforced Polyamide 6, Injection Molding ResinInformation provided by Eurostar. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
Elisto THERMOSTAR® LC 400 GL Insulation Material Pattern material. Insulation materials for mechanical engineering.Information provided by elisto |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROMID 6 G Polyamide 6 Cast This material has good machinability and can be bonded or welded. Its applications include sliding bearings, hammerheads, and toothed gears.Information provided by CENTROPLAST Engineering Plastics .. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | ASTM E 1530 |
Arlon R35928R015 0.0155" (0.394 mm) Uncured/Cured Silicone Rubber with Fiberglass Substrate Design/Construction:Interleave: Polyethylene Side 1, Layer 2: Uncured Silicone RubberSide 1, Layer 1: Cured Silicone Rubber Substrate: Style 7628 Fiberglass Side 2: Cured Silicone RubberAppearance: .. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | |
CENTROPLAST CENTROLYTE ZX Polyethylene terephthalate with lubricant This material's solid lubricant additive has good sliding properties, and is well suited for high load, dry running situations. Possible uses include precision plain bearings, plug connectors, r.. |
|||
Thermal Conductivity | 0.290 W/m-K | 2.01 BTU-in/hr-ft²-°F | Average; ISO 22007-4 |
Victrex® PEEK 381G Medium Viscosity Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, depth filtered granules for specialty extrusion processes, standard flow, FD.. |