Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics EXTEM UH1006 TPI Blend High Heat Amorphous TPI Blend, Excellent Chemical Resistance, High Continuous Use Temperature (CUT), Best-in-class FR, OSU and LOI. Material is UL-listed. This material is RoHS compliant and also ha.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | |
Dow Isoplast® 302 Polyurethane (PUR-RT), Clear Amorphous Polymer
(discontinued **) ISOPLAST® 302 resin is a clear amorphous polymer with the chemical resistance of crystalline resins. Its outstanding properties include clarity, excellent chemical resistance, toughness and high he.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.59 BTU-in/hr-ft²-°F | |
Honeywell ACLAR® 22C (2.00 mil) Copolymer Film
(discontinued **) Description: ACLAR® 22C is a copolymer film consisting primarily of chlorotrifluoroethylene (CTFE). It has moisture barrier and is used for electroluminescent lamps.Information provided by Honeywe.. |
|||
Thermal Conductivity | 0.230 - 0.280 W/m-K | 1.60 - 1.94 BTU-in/hr-ft²-°F | Average value: 0.252 W/m-K Grade Count:3 |
Overview of materials for Nylon 66, Extruded This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, Extruded". Each property range of values reported is minimum and maximum values of appropriate.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1200-7116 ABS, with carbon fiber Applications: Office communication.Electrically conductive, suitable for continuous discharging of statically generated electricity.Information provided by Lehmann & Voss & Co.KG |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1t-7503 Polyamide 6/6T, with PTFE, lubricant modified Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |
|||
Thermal Conductivity | >= 0.230 W/m-K | >= 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
LG Chemical LUCON PO-3000 Electrically Conductive Thermoplastic LG Chemicals has formulated a diverse range of LUCON thermoplastic compounds containing conductive additives, such as carbon powder, (nickel coated) carbon fiber, or stainless steel fiber for solvin.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C-177 |
Glastic GLASTHERM HT250 Insulation Sheet Glastherm Grade HT250 is a high compressive strength, heat-resistant composite material. It is ideal for insulation between the fold and the press or within the mold itself. Grade HT250 is asbesto.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL SE1 PPE+HIPS (Europe-Africa-Middle East) NORYL SE1 is an unfilled, flame retardant material with a Vicat B/120 of 140°C according ISO 306. NORYL SE1 is V1 at 1.47 mm according UL94 and halogen free according VDE/DIN 472 part 815. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Schwartz Technical Plastics LAMIGAMID® 100 Polyamide 6, Extruded, Dry Application: machine parts under 80 mm diameter, hammer-heads, cup-shaped bearing shellsInformation provided by Schwartz Technical Plastics GmbH |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM AUT195 PEI+PCE (Europe-Africa-Middle East) High flow Polyetherimide blend for automotive lighting applications where highly metallized, reflective surfaces are required. Haze onset temperature of 195C (SABIC test method). |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX HX8300HP PC+POLYESTER (Europe-Africa-Middle East) Medium flow, Transparent PC/Polyester alloy. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), food contact compliant... |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX X8300 PC+POLYESTER PC+Polyester, UV Stabilized, Transparent |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics XYLEX X8409AC PC+POLYESTER (Asia Pacific) PC + Polyester, Injection (Blow) Molding, or Extrusion Blow molding grade, Chemical Resistance and Transparency |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX914 PPE+PA (Asia Pacific) NORYL GTX914 is an unfilled GTX grade with an ideal combination of impact performance, dimensional stability at elevated temperatures, chemical resistance and processability. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL GTX GTX934 PPE+PA (Europe-Africa-Middle East) NORYL GTX934 is an unfilled GTX grade with improved processability and heat ageing performance. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics NORYL GTX GTX964W PPE+PS+PA Noryl GTX* GTX964W resin is a blend of Polyphenylene Ether and Polyamide resin with very high impact and high flow. The material wsa designed for large parts, body panels, and thinwall applications.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Noryl HIN120P PPE+HIPS (Europe-Africa-Middle East) Noryl HIN120P is designed for selected one layer water-based paint systems. Noryl HIN120P has a Vicat B/120 of 120 °C and is targetedThis data was supplied by SABIC-IP for the Europe-Africa-Middl.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL PX1134 PPE+HIPS (Europe-Africa-Middle East) NORYL PX1134 is an unfilled material with a Vicat B/120 of 120°C according ISO 306. NORYL PX1134 offers improved impact performance to meet the standard ECE dashboard impact tests in the automoti.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | |
Hippe PA 12 Nylon 12 Maintenance-free bearing and gear components under water, insulated components, seals, gear wheels. Parts for pumps and household units. Application in the electrical sector - less water absorptio.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | |
Hippe PA 6 Nylon 6 Very tough, even at low temperatures. Hard. High attenuation properties. Technical components such as gear wheels, pinions, screws, nuts, bearings, seals, cloth components, guide components, pump.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 125 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 257 °F |
|
Dow SiLK™ I 820 Semiconductor Dielectric Resin SiLK™ I 820 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I 820 is compatible with.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 125 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 257 °F |
|
Dow SiLK™ I300 280 Semiconductor Dielectric Resin SiLK™ I300 280 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 280 is compatibl.. |
|||
Thermal Conductivity | 0.230 W/m-K @Temperature 125 °C |
1.60 BTU-in/hr-ft²-°F @Temperature 257 °F |
|
Dow SiLK™ I300 380 Semiconductor Dielectric Resin SiLK™ I300 380 is designed for easy integration and extendibility, and its formulations offer a robust feature set. High thermal stability and fracture toughness means SilK™ I300 380 is compatibl.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Ultramid® KR 4350 BK 00464 PA6/6T (Dry) Description: For injection-molding and extrusion, exhibiting high toughness, strength and stiffness, low water absorption, high melting point (295 °C [563°F]). The mechanical properties remain con.. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon PA 6 Polyamide 6 General use for mechanical partsGood heat resistanceEasy to useHigh moisture regainInformation provided by Isoflon. |
|||
Thermal Conductivity | 0.230 W/m-K | 1.60 BTU-in/hr-ft²-°F | DIN 52612 |
Lehmann & Voss LUVOCOM® 1-7497 Polyamide 66, with PTFE, lubricant modified, heat stabilized Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.Improved friction and wear behaviour. Emergency running property.Isotropic shrinkage characteri.. |