Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | |
Rotuba 855, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | |
Rotuba 856, Slow Burning Ethyl Cellulose Data provided by the manufacturer. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics EXTEM VH1003M PEI Copolymer Transparent, Thermoplastic Polyimide (TPI) resin with a glass transition temperature (Tg) of 247C. Internal mold release. This product has thinwall FR capability and has a UL94 V0 listing. This mate.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Lexan® 1278R PC (Europe-Africa-Middle East) LEXAN 1278R is a medium viscosity, 20% glass reinforced, flame retardant grade, offering a very high rigidity. It is especially designed for applications like industrial enclosures and fuse boxes re.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 3413R PC 30% GR, provides improved mechanical properties and UL94V-1 rated at 0.058"". Internal mold release added. |
|||
Thermal Conductivity | 0.220 - 400 W/m-K | 1.53 - 2780 BTU-in/hr-ft²-°F | Average value: 78.8 W/m-K Grade Count:12 |
Overview of materials for Epoxy/Carbon Fiber Composite This property data is a summary of similar materials in the MatWeb database for the category "Epoxy/Carbon Fiber Composite". Each property range of values reported is minimum and maximum values of a.. |
|||
Thermal Conductivity | 0.220 - 0.558 W/m-K | 1.53 - 3.87 BTU-in/hr-ft²-°F | Average value: 0.338 W/m-K Grade Count:28 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon PFA Polyperfluoroalkoxyethylene Fluoropolymer material specifications.Information provided by Isoflon. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon PP Polypropylene Products with excellent friction, anti-stick, abrasion and chemical inertia characteristicsVery good impact resistanceNo moisture regainProduct for the food industryInformation provided by Isoflon. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C 177 |
SABIC Innovative Plastics Ultem 1000M PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Americas region. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C 177 |
SABIC Innovative Plastics Ultem 1000M PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1000P PEI Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1000P PEI (Asia Pacific) Standard flow Polyetherimide (Tg 217C) in 350 micron powder. ECO Conforming. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1000R PEI Standard flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, UL94 V0, V2 and 5VA listing. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C 177 |
SABIC Innovative Plastics Ultem 1100EF PEI (Europe-Africa-Middle East) Enhanced flow Polyetherimide (Tg 217C) with internal mold release. ECO Conforming, U.S. FDA and EU Food Contact compliant.This data was supplied by SABIC-IP for the Europe-Africa-Middle East region.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Solvay Specialty Polymers AvaSpire® AV-848 Polyaryletherketone (PAEK) AvaSpire® AV-848 is a high-temperature, polyaryletherketone (PAEK) that offers several key performance advantages over comparable grades of PEEK above 150°C, including better dimensional stabi.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics Ultem XH6050 PEI Copolymer (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).This data was su.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM E 1530 |
SABIC Innovative Plastics Ultem XH6050M PEI Copolymer (Europe-Africa-Middle East) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774).Thi.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL N110HG PPE+HIPS (Europe-Africa-Middle East) NORYL N110HG is an unfilled material, with a Vicat B/120 of 116°C according ISO 306. NORYL N110HG can be used in applications where high gloss is required. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1000E PEI (Europe-Africa-Middle East) Transparent, standard flow Polyetherimide (Tg 217C) with internal mold release. Resin is RoHS compliant. US FDA and EU Food Contact compliant. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics NORYL 731 PPE+HIPS (Europe-Africa-Middle East) NORYL 731 is an unfilled material, with a Vicat B/120 of 140C according ISO 306. NORYL 731 is a general purpose material with good balance of Strength, Impact and Flow. NORYL 731 is available in all.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Westlake Plastics Tempalux® Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high strength at elevated temperatures, high modulus, and broad .. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
Covestro Makrolon® 8325 Polycarbonate High viscosity injection molding and extrusion grade with 20% standard glass fibers and easy mold release, high strength and stiffness.Information provided by Bayer.As of 1 September 2015, Bayer Mat.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 40.0 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 104 °F |
ISO 8302 |
Ensinger TECASINT 1011 Polyimide (PI) TECASINT is a range of non-melting high temperature polyimides characterized by high strength over a wide range of temperatures, good long term thermal stability, minimal thermal expansion and excel.. |
|||
Thermal Conductivity | 0.220 W/m-K @Temperature 40.0 °C |
1.53 BTU-in/hr-ft²-°F @Temperature 104 °F |
ISO 8302 |
Ensinger TECASINT™ 2011 Polyimide (PI) TECASINT™ 2000 series of polyimide stock shapes provide a superior combination of high temperature and bearing and wear, properties that make it an ideal choice for the most demanding applications... |
|||
Thermal Conductivity | <= 0.220 W/m-K | <= 1.53 BTU-in/hr-ft²-°F | ASTM C177/C518 |
Braskem PCD 0140 HECO Polypropylene Heterophasic Copolymer PCD 0140 is a low melt flow rate heterophasic copolymer with high impact resistance. This resin was developed for steel pipe coating extrusion. PCD 0140 is highly protected against thermal aging and.. |
|||
Thermal Conductivity | <= 0.220 W/m-K | <= 1.53 BTU-in/hr-ft²-°F | ASTM C177/C518 |
Braskem PCD 0140BR HECO Polypropylene Heterophasic Copolymer PCD 0140BR is a low melt flow rate heterophasic copolymer with high impact resistance. This resin was developed for steel pipe coating extrusion. PCD 0140BR is highly protected against thermal aging.. |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C 177 |
Adamas Adalon® 992 Modified PTFE Information provided by Adamas, HPM |
|||
Thermal Conductivity | 0.220 W/m-K | 1.53 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics ULTEM 1000 PEI Transparent, standard flow Polyetherimide (Tg 217C). ECO Conforming, UL94 V0, V2 and 5VA listing. US FDA and EU Food Contact compliant, NSF 51 listing, compliant in natural color. Effective June, 20.. |