Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Cycoloy® C8080REC PC+ABS (Europe-Africa-Middle East) PC+ABS, Industrial quality resin with good flow, good temperature resistance and moderate ImpactThis data was supplied by SABIC-IP for the Europe-Africa-Middle East region. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Lexan® 4501 PC (Europe-Africa-Middle East) LEXAN 4501 is a copolymer of polyphthalate carbonate resin for applications requiring high heat resistance. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Lexan® 500R PC (Europe-Africa-Middle East) LEXAN 500R is a medium viscosity, 10% glass reinforced, flame retardant grade, especially designed for applications requiring high rigidity together with high heat resistance and excellent impact pe.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Lexan® 500RS PC (Europe-Africa-Middle East) LEXAN 500RS is a medium viscosity, glass reinforced, flame retardant grade. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Lexan® 505R PC Lexan* 505R Polycarbonate (PC) resin is a 10% glass fiber filled, injection moldable grade. Lexan 505R contains non-chlorinated, non-brominated flame retardant systems with UL-94 V0 rating at 1.5mm... |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® HPH4504 PPC (Europe-Africa-Middle East) High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® HPH4504H PPC (Asia Pacific) High heat specialty polycarbonate with enhanced autoclavability. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 of USP Class VI). EtO, .. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® HPH4704 PPC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C 177 |
SABIC Innovative Plastics Lexan® PPC4701R PPC High heat resistant polyphthlate carbonate, provides DTUL of 300F at 264 psi. Internal mold release.This data was supplied by SABIC-IP for the Americas region. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Lexan® PPC4704 PC (Europe-Africa-Middle East) High heat resistant polycarbonate copolymer, provides of 165 C at 1.82 MPa. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported with bi.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C 177 |
SABIC Innovative Plastics Lexan® PPC4704 PPC High heat resistant polycarbonate copolymer, provides DTUL of 300F at 264 psi. FDA food contact compliant in limited colors. Effective January 15th, 2008 this grade will no longer be supported wit.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman EASTALLOY Polymer DA003-8999K, Clear Alloy
(discontinued **) Properties below based on a film thickness of 250 microns. CO2 Permeability is 49 cm3·mm/m2·24h·atm per ASTM D 1434.Product Description: EASTALLOY DA003-8999K Polymer is a clear copolyester/pol.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® HPH4404 PPC+PC High heat specialty polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO, steam, gamma and e-beam steril.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C177 |
Covestro Apec® DP9-9351 High-Heat Polycarbonate, General Purpose
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C177 |
Covestro Apec® DP9-9354T High-Heat Polycarbonate, Transparent, Flame-Retardant
(discontinued **) Information provided by Bayer Corporation, Plastics DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and has officially adopted its new name – Covestro. This produ.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics PC Polycarbonate Polycarbonate shows a high rigidity and an extreme impact strength. Also it has a high glass transition temperature and temperature resistance. The operating temperature ranges from -60°C to appr.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | DIN 52612 |
Isoflon PC Polycarbonate Good impact resistance among transparent materialsInformation provided by Isoflon. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | |
Momentive Performance Materials N-Sil® RTV128 Silicone Modified Alkoxy Adhesive Sealants, Translucent N-Sil® adhesive sealants are one-component, ready-to-use, and cure to a tough, resilient silicone rubber on exposure to atmospheric moisture at room temperature.Key Performance Properties: Primer.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | |
Momentive Performance Materials RTV142 White, Low Volatile, One Component Silicone Sealant RTV 142 one-component, ready-to-use adhesive sealant cures to a tough, durable, resilient silicone rubber on exposure to atmospheric moisture at room temperature. Methyl alcohol vapors are released.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM 1010F PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). Resin is RoHS compliant. UL94 V0 and 5VA listing. US FDA and EU Food Contant compliant. Effective June, 2007 this grade will no longer be support.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics ULTEM HU1010 PEI (Europe-Africa-Middle East) Transparent, enhanced flow Polyetherimide (Tg 217C). RoHS compliant. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO 10993 or USP Class VI), .. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | |
Shin-Etsu Silicones KE-347T Silicone, RTV Coating Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | |
Shin-Etsu Silicones KE-44 Silicone, RTV Information Provided by Shin-Etsu Silicones of America, Inc. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C177 |
Eastman Drystar 0601 Copolyester, Injection Molded This product-line is designed to meet the needs of converters seeking value-added solutions to their drying requirements of copolyesters. Eastman’s copolyesters are highly valued for their excellen.. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | of melt |
DuPont Performance Polymers Crastin® FGS600F40 NC010 Polybutylene Terephthalate (PBT)
(Unverified Data**) Unreinforced Low Viscosity Polybutylene Terephthalate Developed for Food Contact Applications Crastin FGS600F40 NC010 is an unreinforced low viscosity polybutylene terephthalate resin for injection .. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | |
Hippe PBT Polybutylene Terephthalate The mechanical properties of PBT are generally inferior to the partially crystallized PET, however, PBT is more easily machined.Information provided by Hippe. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C177 |
Asahi Kasei Delpet® 60N Acrylic Molding Compound 60N is a medium grade of heat resistance and mechanical strength, allowing injection molding through relatively small gates and runners. General Delpet® qualities include attractive transparency, .. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® 3412R PC 20% GR, provides improved mechanical properties and UL94 V-1 rated at 0.058"". Internal mold release added. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ASTM C177 |
Kleerdex Elson® 405 AS DC Plate, PMMA/Acrylic, Clear Transparent
(discontinued **) Information provided by Kleerdex Company. Kleerdex Company became KYDEX, LLC in 2009. |
|||
Thermal Conductivity | 0.210 W/m-K | 1.46 BTU-in/hr-ft²-°F | ISO 8302 |
SABIC Innovative Plastics Geloy FXW710SK ASA/SAN (Europe-Africa-Middle East) GELOY FXW710SK is an ASA/SAN injection moulding grade. It is suitable for those applications that require sparkle colour effects.This data was supplied by SABIC-IP for the Europe-Africa-Middle East .. |