Thermal Properties Metric English Comments
Thermal Conductivity 0.186 W/m-K
1.29 BTU-in/hr-ft²-°F
Quadrant EPP Quadrant 1000 LSP PC Extruded Unfilled Polycarbonate
Thermal Conductivity 0.186 W/m-K
1.29 BTU-in/hr-ft²-°F
ASTM F433
Quadrant EPP Quadrant PC 1000 Extruded, Unfilled, Polycarbonate (ASTM Product Data Sheet)
Thermal Conductivity 0.186 W/m-K
1.29 BTU-in/hr-ft²-°F
ASTM F433
Quadrant EPP Quadrant LSG PC (ASTM Product Data Sheet)