Thermal Properties Metric English Comments
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
Melt
Covestro Apec® DP 1-9359/5 Polycarbonate  (discontinued **)
Key Features:Release agentUnfilledSuitable processing methods:Injection moldingThermoformingInformation provided by Bayer Polymers.As of 1 September 2015, Bayer MaterialScience was separated from Ba..
Thermal Conductivity 0.167 - 0.795 W/m-K
1.16 - 5.52 BTU-in/hr-ft²-°F
Average value: 0.480 W/m-K Grade Count:20
Overview of materials for Epoxy, Cast, Unreinforced
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr..
Thermal Conductivity 0.167 - 1.44 W/m-K
1.16 - 10.0 BTU-in/hr-ft²-°F
Average value: 0.838 W/m-K Grade Count:12
Overview of materials for Epoxy, High Temperature
This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Encapsulating, Mineral Filled". Each property range of values reported is minimum and maximum val..
Thermal Conductivity 0.167 - 0.300 W/m-K
1.16 - 2.08 BTU-in/hr-ft²-°F
Average value: 0.292 W/m-K Grade Count:16
Overview of materials for Polytetrafluoroethylene (PTFE), Extruded
This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Extruded". Each property range of values reported is minimum and maximum..
Thermal Conductivity 0.167 - 0.300 W/m-K
1.16 - 2.08 BTU-in/hr-ft²-°F
ASTM C177
Zeus PTFE Tubing
Zeus offers a wide range of standard size products and precision custom PTFE Tubing. PTFE Tubing has become the gold standard in industries requiring the ultimate in lubricity, high temperature use,..
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
Melt
Covestro Apec® 1800 Polycarbonate
Basic gradesoftening temperature (VST/B 120)=185 °CPreprocessingMax. Water content
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
Melt
Covestro Apec® 1803 Polycarbonate
UV-stabilizedsoftening temperature (VST/B 120)=184 °CPreprocessingMax. Water content
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
Melt
Covestro Apec® 1895 Polycarbonate
Easy flowingeasy to demoldsoftening temperature (VST/B 120)=183 °CPreprocessingMax. Water content
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
Melt
Covestro Apec® 1897 Polycarbonate
Easy flowingeasy to demoldUV-stabilizedsoftening temperature (VST/B 120)=182 °CPreprocessingMax. Water content
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
Melt
Covestro Apec® DP1-9354 Polycarbonate, Flame Retardant Grade
Developmental productflame retardant: V-0/1,5mm (UL 94)V-0/3,0mm (UL 94)5VA/3mm (UL 94)softening temperature (VST/B 120)=185 °Conly opaque colors availablePreprocessingMax. Water content
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
Melt
Covestro Apec® DP1-9354/1 Polycarbonate, Flame Retardant Grade
Developmental productflame retardant: V-0/3,2mm (UL 94)V-2/1,5mm (UL 94),softening temperature (VST/B 120)=185 °Calso available in transparent colorsPreprocessingMax. Water content
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
Melt
Covestro Makroblend® KU 2-7912/5 Polycarbonate + PBT, Impact Grade
Developmental productISO 7792-1-PBT/PC,MHPR,-020(PC+PBT)-blendsimpact modifiedInjection molding gradehigh flowhigh toughness at low temperaturesunreinforcedPreprocessingMax. Water content
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Abatron AboCast/AboCure 50-24/8501-4 High Temperature Resistant Epoxy
Clear amber, low viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components to..
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Abatron AboCast/AboCure 8502-1 Epoxy
AboCast/AboCure 8502-1 is a solventless clear Epoxy System, used as a casting, adhesive, and impregnating resin for transformers, capacitors, coils, and other electronic components requiring a low-v..
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Abatron AboCast 8103-13 One-Component Epoxy
AboCast 8103-13 is the low-viscosity one-component clear epoxy system with deep impregnation that offers high performance at relatively high temperatures. It is best for thin-wall casting. Suggested..
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Abatron AboCast 8501-6 One-Component Epoxy
AboCast 8501-6 is a clear, high-temperature one-component epoxy system for very high-temperature uses. It offers the highest heat resistance of the clear resins. Suggested Uses: Casting; Potting; E..
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Abatron AboCast 8504-1 One-Component Epoxy
AboCast 8504-1 is a clear, all-purpose one-component epoxy system, with an optimum balance of properties for most casting, adhesive, impregnation, and coating applications.
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Abatron AboCast 8504-5 One-Component Epoxy
AboCast 8504-5 is a clear, plasticized one-component epoxy system with very high strength and impact. It provides exceptional physical properties and thermal shock resistance from sub-zero to modera..
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Abatron AboCast/AboCure 8501-6/8501-4 High Temperature Resistant Epoxy
1-component system. Clear amber, low viscosity, structural/dielectric epoxy.Processing: Pot Life: 5-9 months. Cured 2 hours at 95°C + 15 hour post-cure at 230°C. Information provided by Abatron...
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
BS 874A
Mitsui TPX® DX820 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
BS 874A
Mitsui TPX® MX002 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
BS 874A
Mitsui TPX® MX004 Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
BS 874A
Mitsui TPX® RT18 Methylpentene Copolymer, Transparent Grade
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Thermal Conductivity 0.167 W/m-K
1.16 BTU-in/hr-ft²-°F
BS 874A
Mitsui TPX® RT18 XB Methylpentene Copolymer
TPX® is a 4-methylpentene-1 based polyolefin with a unique combination of transparency, heat and chemical resistant qualities. TPX is used in a wide variety of applications, including: medical equi..
Thermal Conductivity 0.167 - 0.201 W/m-K
1.16 - 1.39 BTU-in/hr-ft²-°F
Abatron AboCast/AboCure 50-7/8501-4 High Temperature Resistant Epoxy
Clear amber, high viscosity, structural/dielectric epoxy with high temperature resistance.Suggested Uses: Casting, bonding, potting, encapsulation of electric, structural and industrial components t..