Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.130 W/m-K | 0.902 BTU-in/hr-ft²-°F | ASTM C177 |
Plaskolite Optix® Acrylic Sheet Optix® is a continuously processed acrylic sheet that is crystal clear, impact resistant, weather resistant, and non-yellowing. It offers high molecular weight for superior thermoforming, bending,.. |
|||
Thermal Conductivity | 0.130 W/m-K | 0.902 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® FL910 PC Various weight reductions at 0.250"" (6.35 mm) wall, 10% GR. High flexural strength and modulus, impact/heat resistant. V-0/5V at 0.250"" (6.35 mm). |
|||
Thermal Conductivity | 0.130 W/m-K | 0.902 BTU-in/hr-ft²-°F | ASTM C177 |
SABIC Innovative Plastics Lexan® FL913 PC Various weight reduction at 0.250"" (6.35 mm) wall. 10% GR, high flexural strength/modulus. UL rated V-0/5VA (all except natural). UV-stabilized. |
|||
Thermal Conductivity | 0.130 W/m-K | 0.900 BTU-in/hr-ft²-°F | ASTM C177 |
Plaskolite Optix® DA Digital Acrylic Sheet Designed to provide optimal adhesion of UV curing inks without adhesion promoters, OPTIX DA is a continuously processed acrylic sheet specially formulated product for printing. OPTIX DA provides sup.. |
|||
Thermal Conductivity | 0.130 W/m-K | 0.902 BTU-in/hr-ft²-°F | DIN 52612 |
GEHR Plastics PVDF Polyvinylidene Fluoride Polyvinylidene fluoride shows a higher tensile strength, pressure resistance and dimensional stability than the related PTFE, but friction and insulation properties are lower. PVDF has a high mechan.. |
|||
Thermal Conductivity | 0.130 W/m-K | 0.902 BTU-in/hr-ft²-°F | Melt; ASTM C177 |
Styron MAGNUMâ„¢ 357 HP Acrylonitrile Butadiene Styrene (ABS) Resin Overview: MAGNUMâ„¢ ABS resins are thermoplastic materials which provide an excellent balance of processability, impact resistance and heat resistance as imparted by the various polymer compositi.. |
|||
Thermal Conductivity | 0.130 W/m-K @Temperature 650 °C |
0.902 BTU-in/hr-ft²-°F @Temperature 1200 °F |
ASTM-C177 |
Unifrax CC-Max® 4 HP Substrate Support Mat CC-Max 4 HP mat is produced when the proprietary fiber is converted into a flexible flet-like product. The material is thermally stable and engineered to maintain a controlled holding force on the .. |
|||
Thermal Conductivity | 0.130 W/m-K | 0.902 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Cast 3110 Low Density Epoxy Casting System TRA-CAST 3110 is a unicellular, low density, syntactic-foam epoxy resin casting system of medium viscosity that easily handles, mixes and cures at room temperature. Developed for industrial encapsul.. |
|||
Thermal Conductivity | 0.130 W/m-K | 0.902 BTU-in/hr-ft²-°F | |
Trelleborg Offshore Vikotherm™ 73585 Insulative Elastomer Vikotherm™ is a rubber elastomer chemically modified to provide very high insulating characteristics while maintaining its inherent rubber properties in respect of seawater resistance, pressure res.. |
|||
Thermal Conductivity | 0.130 W/m-K | 0.902 BTU-in/hr-ft²-°F | |
Tra-Con Tra-Bond 2125 Rigid Syntactic Repair Adhesive TRA-BOND 2125 is a medium viscosity, low density syntactic foam epoxy formulation developed for industrial, electronic and aerospace honeycomb, fillet, edge-fill, contour repair, bonding and casting.. |
|||
Thermal Conductivity | 0.130 W/m-K | 0.902 BTU-in/hr-ft²-°F | |
CMT Materials HYTAC® C1R Highly Durable Syntactic Foam, Dust-Free Machining/Polishing HYTAC-C1R is easily machined without the dust typically associated with epoxy syntactic foam. This new copolymer base has been optimized for both the machine shop and the thermoforming process.Exce.. |
|||
Thermal Conductivity | 0.130 - 0.170 W/m-K | 0.902 - 1.18 BTU-in/hr-ft²-°F | |
Abatron AboCast/AboCure 8109-11 All-purpose, structural dielectric resin. Better thermal and chemical properties than 8109-8, but requires heat cure. Melts at 70-80°C and remains liquid (supercooled) for many hours at RT.Process.. |
|||
Thermal Conductivity | 0.130 - 0.190 W/m-K | 0.900 - 1.32 BTU-in/hr-ft²-°F | Average value: 0.160 W/m-K Grade Count:4 |
Overview of materials for Acrylic, Optical Sheet This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Optical Sheet". Each property range of values reported is minimum and maximum values of appropr.. |