Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0460 W/m-K | 0.319 BTU-in/hr-ft²-°F | mean temp of 80°C; ASTM C 518 |
Zotefoams ZOTEK® F OSU Flexible PVDF Foam Zotek® F OSU is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and .. |
|||
Thermal Conductivity | 0.0460 W/m-K | 0.319 BTU-in/hr-ft²-°F | mean temp of 80°C; ASTM C 518 |
Zotefoams ZOTEK® F 30 PVDF Foam Zotek® F 30 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Thermal Conductivity | 0.0460 W/m-K | 0.319 BTU-in/hr-ft²-°F | mean temp of 80°C; ASTM C 518 |
Zotefoams ZOTEK® F 35 PVDF Foam Zotek® F 35 is a closed cell foam made from Arkema Kynar® PVDF manufactured using nitrogen expansion technology to produce foams with exceptional cell size uniformity, low odor / high purity and o.. |
|||
Thermal Conductivity | 0.0460 W/m-K | 0.319 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9270 0.1 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0460 W/m-K | 0.319 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9280 0.1 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0460 W/m-K | 0.319 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9280 0.11 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9280 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9280.Note: In order to mea.. |
|||
Thermal Conductivity | 0.0460 W/m-K | 0.319 BTU-in/hr-ft²-°F | DIN 52612 |
BASF Neopolen® P 9270 0.11 g/cc Core density; Expanded Polypropylene (Europe) Description: Neopolen® P 9270 is expanded Polypropylene supplied in the form of beads. The cells are largely closed.Physical properties of moldings made from Neopolen® P 9270.Note: In order to mea.. |