Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 30.0 - 103 µm/m-°C | 16.7 - 57.0 µin/in-°F | Average value: 68.7 µm/m-°C Grade Count:7 |
Overview of materials for ABS/Polyester Alloy This property data is a summary of similar materials in the MatWeb database for the category "ABS/Polyester Alloy". Each property range of values reported is minimum and maximum values of appropriat.. |
|||
CTE, linear | 45.0 - 103 µm/m-°C | 25.0 - 57.0 µin/in-°F | Average value: 73.5 µm/m-°C Grade Count:5 |
Overview of materials for Polytetrafluoroethylene (PTFE), Mica Filled This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Mica Filled". Each property range of values reported is minimum and maxi.. |
|||
CTE, linear | 30.0 - 103 µm/m-°C | 16.7 - 57.0 µin/in-°F | Average value: 58.5 µm/m-°C Grade Count:30 |
Overview of materials for Nylon 6, 30% Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, 30% Mineral Filled". Specific grades with primary filler content between 25% and 34% are includ.. |