Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 3.24 - 88.0 µm/m-°C | 1.80 - 48.9 µin/in-°F | Average value: 40.3 µm/m-°C Grade Count:33 |
Overview of materials for Polycarbonate, 10% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 10% Glass Filled". Specific grades with glass content between 5% and 14% are included. Ea.. |
|||
CTE, linear | 41.0 - 88.0 µm/m-°C @Temperature 50.0 - 300 °C |
22.8 - 48.9 µin/in-°F @Temperature 122 - 572 °F |
Average value: 61.0 µm/m-°C Grade Count:3 |
Overview of materials for Thermoplastic Polyimide, Carbon Fiber This property data is a summary of similar materials in the MatWeb database for the category "Thermoplastic Polyimide, Carbon Fiber". Each property range of values reported is minimum and maximum va.. |