Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 55.0 - 75.0 µm/m-°C | 30.6 - 41.7 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP EIP12030F Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 55.0 - 75.0 µm/m-°C | 30.6 - 41.7 µin/in-°F | Polykemi |
Polykemi AB POLYfill PP EIP12030RF Polypropylene/EPDM, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 59.9 - 75.0 µm/m-°C | 33.3 - 41.7 µin/in-°F | Average value: 65.0 µm/m-°C Grade Count:3 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 49.0 - 75.0 µm/m-°C @Temperature 40.0 - 130 °C |
27.2 - 41.7 µin/in-°F @Temperature 104 - 266 °F |
Average value: 62.0 µm/m-°C Grade Count:2 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
CTE, linear | 72.0 - 75.0 µm/m-°C | 40.0 - 41.7 µin/in-°F | Average value: 74.4 µm/m-°C Grade Count:5 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
CTE, linear | 70.0 - 75.0 µm/m-°C | 38.9 - 41.7 µin/in-°F | |
Master Bond MB250NT Low viscosity ethyl cyanoacrylate Master Bond MB250NT is a single component ethyl cyanoacrylate type system. This rapid curing, high strength system is used primarily in applications where the ISO 10993-5 for low toxicity is specifi.. |
|||
CTE, linear | 70.0 - 75.0 µm/m-°C | 38.9 - 41.7 µin/in-°F | |
Master Bond MB306 Low Viscosity Methyl Cyanoacrylate Features superior bonding properties. Master Bond MB306 is a single component, low viscosity, rapid setting, methyl cyanoacrylate adhesive. Similar to other types of “super glue”, MB306 cures ver.. |
|||
CTE, linear | 74.5 - 75.1 µm/m-°C | 41.4 - 41.7 µin/in-°F | |
Cast Nylons Nycast® SLX Premium Bearing Grade Nylon Nycast® SLX closes the gap between static and dynamic coefficients of friction. Used in wear pads, bearing blocks, and other load-bearing slide applications.Data provided by the manufacturer, Cast.. |
|||
CTE, linear | 50.0 - 75.0 µm/m-°C | 27.8 - 41.7 µin/in-°F | Polykemi |
Polykemi AB POLYfill PPH TS5040 Polypropylene Homopolymer, Mineral Reinforced Information provided by Polykemi AB |
|||
CTE, linear | 55.0 - 75.0 µm/m-°C @Temperature -30.0 - 30.0 °C |
30.6 - 41.7 µin/in-°F @Temperature -22.0 - 86.0 °F |
TMA |
SABIC Innovative Plastics NORYL EX130 PPE+HIPS (Asia Pacific) PPE+PS Auto Exterior Grade |