Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.80 - 8.50 µm/m-°C @Temperature 20.0 - 100 °C |
4.33 - 4.72 µin/in-°F @Temperature 68.0 - 212 °F |
|
MarkeTech W80Cu Tungsten/Copper Heat Sink Material WCu composites are made by vacuum infiltration of uniform controlled porous blocks of tungsten with molten copper. This results in a material with an interconnected Cu matrix that has high thermal c.. |
|||
CTE, linear | 4.00 - 8.50 µm/m-°C @Temperature 1000 °C |
2.22 - 4.72 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories CUN-846 Nozzle Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 7.60 - 8.50 µm/m-°C @Temperature 25.0 - 800 °C |
4.22 - 4.72 µin/in-°F @Temperature 77.0 - 1470 °F |
|
China-Yixing Longly Refractories 99 Alumina Ceramic Seals LONGLY's alumina ceramic seals (alumina accounts for 95-99%) can be finished by mirror-polishing process. Because of high mechanical strength, strong chemical corrosion resistance, good air tightne.. |
|||
CTE, linear | 7.60 - 8.50 µm/m-°C @Temperature 25.0 - 800 °C |
4.22 - 4.72 µin/in-°F @Temperature 77.0 - 1470 °F |
|
China-Yixing Longly Refractories 99 Alumina Ceramic LONGLY selects high quality ceramic fine powder and micropowder as materials, adopts modern advanced molding technology to produce a multitude of ceramic tubes, rods, beads, balls, columns, plates, .. |