Polymer Property : CTE, linear = 283 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 1.00 - 510 µm/m-°C
0.556 - 283 µin/in-°F
Average value: 161 µm/m-°C Grade Count:43
Overview of materials for Thermoset Polyurethane, Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane, Adhesive". Each property range of values reported is minimum and maximum values ..