Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.3 - 48.6 µm/m-°C | 8.50 - 27.0 µin/in-°F | Average value: 28.0 µm/m-°C Grade Count:23 |
Overview of materials for Nylon 610, Glass Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Nylon 610, Glass Reinforced". Each property range of values reported is minimum and maximum values of ap.. |
|||
CTE, linear | 10.0 - 48.6 µm/m-°C | 5.56 - 27.0 µin/in-°F | Average value: 29.1 µm/m-°C Grade Count:7 |
Overview of materials for Nylon 12, Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 12, Carbon Fiber Filled". Each property range of values reported is minimum and maximum values of .. |
|||
CTE, linear | 16.0 - 48.6 µm/m-°C | 8.89 - 27.0 µin/in-°F | Average value: 25.1 µm/m-°C Grade Count:4 |
Overview of materials for Polybutylene Terephthalate (PBT), Carbon Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polybutylene Terephthalate (PBT), Carbon Fiber Filled". Each property range of values reported is minimu.. |