Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 25.2 - 27.0 µm/m-°C | 14.0 - 15.0 µin/in-°F | Average value: 25.9 µm/m-°C Grade Count:5 |
Overview of materials for Polyetherimide (PEI), 20% Glass Fiber This property data is a summary of similar materials in the MatWeb database for the category "Polyetherimide, 20% Glass Fiber". Specific grades with glass content between 15% and 24% are included. E.. |
|||
CTE, linear | 10.0 - 27.0 µm/m-°C | 5.56 - 15.0 µin/in-°F | Average value: 20.5 µm/m-°C Grade Count:25 |
Overview of materials for Nylon 66, 60% Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Nylon 66, 60% Glass Fiber Filled". Specific grades with glass content between 55% and 64% are included. .. |
|||
CTE, linear | 16.2 - 27.0 µm/m-°C | 9.00 - 15.0 µin/in-°F | Average value: 21.9 µm/m-°C Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), Carbon Fiber + PTFE Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Carbon Fiber + PTFE Filled". Each property range of values reported is minimum and maxi.. |