Thermal Properties Metric English Comments
CTE, linear 0.800 - 1.90 µm/m-°C

@Temperature 20.0 - 1000 °C
0.444 - 1.06 µin/in-°F

@Temperature 68.0 - 1830 °F
China-Yixing Longly Refractories Cordierite Ceramics (Heat Resistance Ceramics)
LONGLY's cordierite ceramics' main crystal phrase is 2MgO-2Al2O2-5SiO2, this composition has low thermal expansion coefficient and excellent thermal shock resistance. Maximum service temperature is..