Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.3 µm/m-°C @Temperature 20.0 - 300 °C |
9.60 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 18665 MSP1, 1/2 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
CTE, linear | 17.3 µm/m-°C @Temperature 20.0 - 300 °C |
9.60 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 18665 MSP1, 1/4 Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
CTE, linear | 17.3 µm/m-°C @Temperature 20.0 - 300 °C |
9.60 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 18665 MSP1, Annealed MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
CTE, linear | 17.3 µm/m-°C @Temperature 20.0 - 300 °C |
9.60 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 18665 MSP1, Extra Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
CTE, linear | 17.3 µm/m-°C @Temperature 20.0 - 300 °C |
9.60 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 18665 MSP1, Hard MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |
|||
CTE, linear | 17.3 µm/m-°C @Temperature 20.0 - 300 °C |
9.60 µin/in-°F @Temperature 68.0 - 572 °F |
|
Eagle Brass 18665 MSP1, Spring MSP-1 high performance copper alloy with magnesium has high conductivity (63% IACS), high strength and excellent thermal creep properties. Typical uses include terminals, connectors, relays, springs.. |