Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 17.0 µm/m-°C | 9.44 µin/in-°F | Y-Direction; IPC-TM-650 2.4.41 |
Rogers Corporation LoPro™ RO4730 Antenna Grade Non-PTFE Laminate RO4730 LoPro Antenna Grade Laminates are fully compatible with conventional FR-4 and high temperature lead-free solder processing. The resin systems of RO4730 dielectric materials are designed to p.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; A (TB00) Temper; All Thicknesses (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; over 51 to 76 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17000) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 165 Plate & Rolled Bar; HT (TH04) Temper; over 51 to 76 mm Thickness (UNS C17000) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 51 to 76 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; up to 9.5 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 51 to 76 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; HT (TH04) Temper; over 9.5 to 25 mm Thickness (UNS C17200) Treatment required for max strength: 2 hrs @ 330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials In.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Rod and Bar; AT (TF00) Temper; over 76 mm (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Material.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; over 9.5 to 25.4 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Strip; 1/2H (TD02) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0.5Formability Ratio (bad Way): 1Superficial Hardness: 30T 74-79Tabulated properties appl.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Strip; A -Dead Soft (TB00) Temper (UNS C17200) Treatment required for max strength: as suppliedFormability Ratio, 90° Bend, Radius/Thickness (Good Way): 0Formability Ratio (bad Way): 0Superficial Hardness: 30T 46-67Tabulated properties apply .. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Tube; HT (TH04) Temper; up to 9.5 mm o.d. (UNS C17200) Treatment required for max strength: 2-3 hrs @ 315-330°C or Mill HardenedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materi.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Wire; AT (TF00) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 3 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; up to 9.5 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy M25 Wire; 1/4H (TD01) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy M25 Wire; 1/4HT (TH01) Temper; 1.3-12.7 mm Diameter (UNS C17300) Treatment required for max strength: 2 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed i.. |
|||
CTE, linear | 17.0 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
9.44 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP660 Paper Base Laminate Description: Lower cost paper phenolic NEMA Grade XP. Uses natural kraft paper without pigmented cover sheet. Warm to hot punching. UL listed. Thickness Tested: 0.062", 0.125" & 0.500" |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Plate & Rolled Bar; H (TD04) Temper; over 25 to 51 mm Thickness (UNS C17200) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy 25 Wire; 1/2HT (TH02) Temper; 1.3-12.7 mm Diameter (UNS C17200) Treatment required for max strength: 1.5 hrs @ 315-330°C Tabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy M25 Rod and Bar; H (TD04) Temper; over 25.4 to 76 mm (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 20.0 - 200 °C |
9.44 µin/in-°F @Temperature 68.0 - 392 °F |
|
Materion Beryllium Copper Alloy M25 Wire; H (TD04) Temper; 1.3-2.0 mm Diameter (UNS C17300) Treatment required for max strength: as suppliedTabulated properties apply to products after age hardening. Information supplied by Brush Wellman.Brush Engineered Materials Inc. changed its name to.. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 30.0 - 50.0 °C |
9.44 µin/in-°F @Temperature 86.0 - 122 °F |
92 Gauge; ASTM D696 |
DuPont Teijin Films Mylar® A Polyester Film, 1000 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 30.0 - 50.0 °C |
9.44 µin/in-°F @Temperature 86.0 - 122 °F |
92 Gauge; ASTM D696 |
DuPont Teijin Films Mylar® A Polyester Film, 750 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
CTE, linear | 17.0 µm/m-°C @Temperature 30.0 - 50.0 °C |
9.44 µin/in-°F @Temperature 86.0 - 122 °F |
92 Gauge; ASTM D696 |
DuPont Teijin Films Mylar® A Polyester Film, 900 Gauge Mylar® A films are tough, general purpose films that are transparent in 48 through 92 gauge and translucent in heavier gauges. They have a rough surface to provide ease of handling, good adhesion, .. |
|||
CTE, linear | 17.0 - 72.0 µm/m-°C | 9.44 - 40.0 µin/in-°F | Average value: 23.9 µm/m-°C Grade Count:24 |
Overview of materials for Polyphthalamide (PPA), 30% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 30% Glass Fiber Reinforced". Specific grades with glass content between 25% and 34% are.. |
|||
CTE, linear | 17.0 - 95.0 µm/m-°C @Temperature 50.0 - 250 °C |
9.44 - 52.8 µin/in-°F @Temperature 122 - 482 °F |
Average value: 45.7 µm/m-°C Grade Count:6 |
Overview of materials for Polyphthalamide (PPA), Mineral Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, Mineral Filled". Each property range of values reported is minimum and maximum values o.. |