Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 16.8 µm/m-°C @Temperature 20.0 - 1000 °C |
9.33 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Kennametal Stellite Stellite® 250 Resistant to heat, thermal shock, thermal cycling, oxidation, and hot corrosion from flue gas, slags, and molten copper. Not recommended for use in abrasive wear.Applications:heat treatment furnace.. |
|||
CTE, linear | 16.8 µm/m-°C @Temperature 20.0 - 1000 °C |
9.33 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Goodfellow T2-Thermocouple Alloy The negative element of the type K thermocouple, the positive being T1. The thermocouple can be used up to 1250C in oxidizing atmospheres, and probably is the most common in use.Information provided.. |