Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 15.8 µm/m-°C @Temperature 20.0 - 649 °C |
8.80 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 1008 Low Carbon Steel, 1/4 Hardened 1008 is a standard grade Carbon Steel. This alloy is generally used for "commercial quality" cold rolled steel. It is an economical, general purpose steel grade offering moderate strength and toughn.. |
|||
CTE, linear | 15.8 µm/m-°C @Temperature 20.0 - 649 °C |
8.80 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 1008 Low Carbon Steel, Full Hardened 1008 is a standard grade Carbon Steel. This alloy is generally used for "commercial quality" cold rolled steel. It is an economical, general purpose steel grade offering moderate strength and toughn.. |
|||
CTE, linear | 15.8 µm/m-°C @Temperature 20.0 - 649 °C |
8.80 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 1008 Low Carbon Steel, 1/2 Hardened 1008 is a standard grade Carbon Steel. This alloy is generally used for "commercial quality" cold rolled steel. It is an economical, general purpose steel grade offering moderate strength and toughn.. |
|||
CTE, linear | 15.8 µm/m-°C @Temperature 20.0 - 649 °C |
8.80 µin/in-°F @Temperature 68.0 - 1200 °F |
|
Eagle Brass 1008 Low Carbon Steel, Annealed 1008 is a standard grade Carbon Steel. This alloy is generally used for "commercial quality" cold rolled steel. It is an economical, general purpose steel grade offering moderate strength and toughn.. |