Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 14.7 µm/m-°C @Thickness 1.57 mm, Temperature 20.0 °C |
8.17 µin/in-°F @Thickness 0.0620 in, Temperature 68.0 °F |
x-axis; IPC-TM 650-2.4.24 |
Industrial Laminates/Norplex NP130HF Glass Fabric Description: High flexural, impact and tensile strength glass fabric epoxy laminate, especially in the machine direction. Engineered to provide better physical properties than NEMA FR-4. More dimens.. |
|||
CTE, linear | 14.7 µm/m-°C @Temperature 20.0 - 100 °C |
8.17 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals FERRY® Alloy A copper-nickel alloy used mainly for its electrical properties. It has medium-range electrical resistivity and a very low temperature coefficient of resistance (TCR). The low TCR makes the alloy .. |
|||
CTE, linear | 14.7 µm/m-°C @Temperature 25.0 - 500 °C |
8.17 µin/in-°F @Temperature 77.0 - 932 °F |
|
Wieland Euro 50 PFM Alloy Gold-palladium ceramic alloyApplications: crowns, short span bridges, long span bridges, telescopic and milling work, ceramic veneering, acrylic veneeringDental |
|||
CTE, linear | 14.7 µm/m-°C @Temperature 20.0 °C |
8.17 µin/in-°F @Temperature 68.0 °F |
|
Williams Advanced Alloys WS487 Solder All Williams alloys are available in a variety of shapes and forms, including ribbon, preforms, rod, ring, wire, and custom shapes.Information provided by Williams Advanced Alloys |
|||
CTE, linear | 14.7 µm/m-°C @Temperature 20.0 - 100 °C |
8.17 µin/in-°F @Temperature 68.0 - 212 °F |
|
Alloy Wire International RW 45 Ni-Cu Resistance Wire Used in thermocouples, power resistors, shunts, and wire wound precision restors up to 750°F (400°C)Information provided by Alloywire International. |
|||
CTE, linear | 14.7 µm/m-°C @Temperature 20.0 - 100 °C |
8.17 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals INCOLOY® Alloy 020 A nickel-iron-chromium alloy with additions of copper and molybdenum. It also contains niobium for stabilization against sensitization and resultant intergranular corrosion. The alloy has excellen.. |