Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 140 µm/m-°C @Temperature 23.0 - 100 °C |
77.8 µin/in-°F @Temperature 73.4 - 212 °F |
|
Quadrant EPP Borotron® HM PE-HMW + boron based additive (ISO Data) Borotron UH and Borotron HM are boron loaded PE-(U)HMW grades, specifically developed for neutron shielding purposes in nuclear installations. The high hydrogen content of PE-(U)HMW makes it very su.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
NOVA Chemicals Novapol® HD-2100-U MDPE Extrusion Resin Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
NOVA Chemicals Novapol® HP-Y353-A HDPE Pipe Coating Resin Good ESCR, Excellent toughness, High strength, Excellent processability, Excellent stiffnessApplications: For profile, corrugated non-pressure pipes, For storm and sanitary sewer pipe, For culvert a.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
NOVA Chemicals Novapol® HD-2100-A MDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, high strength, excellent processability.Applications: pipe, water pipe, fuel gas pipe, re-lining pipe, steel pipe coating.Data provided by the manufacturer. |
|||
CTE, linear | 140 µm/m-°C @Temperature -20.0 - 32.0 °C |
77.8 µin/in-°F @Temperature -4.00 - 89.6 °F |
ASTM D696 |
DuPont™ Surlyn® 8527 Ionomer Resin, Sodium
(discontinued **) Surlyn® 8527 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
CTE, linear | 140 µm/m-°C | 77.8 µin/in-°F | Alpha 2 |
Lord Adhesives CircuitSAFâ„¢ MA-420 Epoxy Surface Mount Adhesive CircuitSAFâ„¢ MA-420 is an epoxy surface mount adhesive that cures rapidly at elevated temperatures and has been designed for use in high speed printed circuit board assembly for the attachment o.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 23.0 - 100 °C |
77.8 µin/in-°F @Temperature 73.4 - 212 °F |
ASTM D696 |
Manifattura Cattaneo PP H Polypropylene Manifattura Cattaneo products are available in semi-finished forms such as bars, profiles, sheets and plates.Information provided by Manifattura Cattaneo s.p.a. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ P150B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ P150B-05 Polyester TPE, Non-smell, Non-deposit Features: Polyester TPE, Non-smell, Non-depositInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo Pelprene™ P-280B Polyester TPE Key Feature: Pelprene P typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'P' type is a block.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ P90B Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ P90BD Polyester TPE, High Viscous, High Durability Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ S2001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ S2004FS Polyester TPE, Flame Resistant Features: Polyester TPE, Flame ResistantInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ S3001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo Pelprene™ S-6001 Polyester TPE Key Feature: Pelprene S typePelprene™ can be processed into a wide variety of articles from ultra-small precision parts to sheets by injection, extrusion, and blow molding. The 'S' type is a block.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ S9001 Polyester TPE Features: Polyester TPEInformation provided by Toyobo. |
|||
CTE, linear | 140 µm/m-°C @Temperature 23.0 - 55.0 °C |
77.8 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® SF-20 Acetal Co-polymer (POM), High impact, Flexible DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 140 µm/m-°C @Temperature 23.0 - 55.0 °C |
77.8 µin/in-°F @Temperature 73.4 - 131 °F |
ISO 11359-2 |
Polyplastics Duracon® SW-01 Acetal Co-polymer (POM), High sliding, Special lubricant, High sliding DURACON® is a crystalline thermoplastic acetal copolymer. The primary raw material trioxane, a trimer of formaldehyde.The thermoplastic adopts a copolymer structure in which polyoxymethylene (-C-O).. |
|||
CTE, linear | 140 µm/m-°C | 77.8 µin/in-°F | Above Tg |
Tra-Con Tra-Bond 789-3TN1 Moisture Resistant Adhesive TRA-BOND 789-3TN1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistanc.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Covestro Bayflex® XGT-16 Polyurethane Elastomeric RIM, MDI-based 2-Component Liquid System 0.125 in. thickness. RIM = Reaction Injection MoldingInformation provided by Bayer Corporation, Polyurethanes DivisionAs of 1 September 2015, Bayer MaterialScience was separated from Bayer AG and of.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
|
Cytec EN-2543 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
CTE, linear | 140 µm/m-°C @Temperature -20.0 - 32.0 °C |
77.8 µin/in-°F @Temperature -4.00 - 89.6 °F |
ASTM D696 |
DuPont™ Surlyn® 8920 Ionomer Resin, Sodium Surlyn® 8920 thermoplastic resin is an advanced ethylene/methacrylic acid (E/MAA) copolymer, in which the MAA acid groups have been partially neutralized with sodium ions. The amount of MAA and neu.. |
|||
CTE, linear | 140 µm/m-°C | 77.8 µin/in-°F | |
Fainplast Compounds EVAtech 801S Ethylene Vinyl Acetate Foam EVA (ethylene-vinyl acetate) designed for the production of crosslinked expanded products using injection technology.Information provided by Fainplast Compounds |
|||
CTE, linear | 140 µm/m-°C @Temperature -40.0 - 140 °C |
77.8 µin/in-°F @Temperature -40.0 - 284 °F |
ASTM D696 |
Arkema Group Pebax® 6333 Polyether Block Amide (PEBA) Information provided by Arkema Group |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
ISO 11359 |
CENTROPLAST CENTRODAL GL Polyoxymethylene + PE-UHMW CENTRODAL GL has good dry running and emergency running properties. During the modification of POM + PE, a PE-UHMW is incorporated to the basic polyoxymethylene polymer. It leads to an improvement.. |
|||
CTE, linear | 140 µm/m-°C @Temperature 20.0 °C |
77.8 µin/in-°F @Temperature 68.0 °F |
TMA |
Toyobo PELPRENE™ S3002 Polyester TPE, Ultra Heat-resistant Features: Polyester TPE, Ultra Heat-resistantInformation provided by Toyobo. |
|||
CTE, linear | 140 - 190 µm/m-°C | 77.8 - 106 µin/in-°F | Average value: 163 µm/m-°C Grade Count:8 |
Overview of materials for High Density Polyethylene (HDPE), Crosslinkable This property data is a summary of similar materials in the MatWeb database for the category "High Density Polyethylene (HDPE), Crosslinkable". Each property range of values reported is minimum and .. |