Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 139 µm/m-°C @Temperature 20.0 °C |
77.2 µin/in-°F @Temperature 68.0 °F |
ASTM E831 |
Spartech Royalite R21M General Purpose ABS Resin Data provided by the manufacturer. A general-purpose ABS resin with high impact strength, R-21M is a popular choice for a variety of products, from bicycle helmets and carrying cases to portable ta.. |
|||
CTE, linear | 139 µm/m-°C | 77.2 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® TV1002 Polyimide Adhesive Material Description: A single component, screen printable polyimide adhesive designed for semiconductor wafer passivation applications. It is a high temperature chemistry capable of resisting >400.. |