Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 132 µm/m-°C @Temperature -50.0 - 100 °C |
73.3 µin/in-°F @Temperature -58.0 - 212 °F |
|
Sorbothane Polyurethane Damping Material, 30 Durometer Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the m.. |
|||
CTE, linear | 132 µm/m-°C @Temperature -50.0 - 100 °C |
73.3 µin/in-°F @Temperature -58.0 - 212 °F |
|
Sorbothane Polyurethane Damping Material, 50 Durometer Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the m.. |
|||
CTE, linear | 132 µm/m-°C | 73.3 µin/in-°F | Above Tg |
Epoxy Technology EPO-TEK® 323LP Epoxy Material Description: Longer pot life version of EPO-TEK® 353ND designed for semiconductor, hybrid, fiber-optic, hard-disk drive and medical applications.Information Provided by Epoxy Technology |
|||
CTE, linear | 132 µm/m-°C | 73.3 µin/in-°F | Below Tg |
3M Scotch-Weld™ DP8010NS Structural Adhesive 3M™ Scotch-Weld™ Structural Plastic Adhesive DP-8010NS is a two-part acrylic-based adhesive (10:1 ratio by volume) that can bond many low surface energy plastics, including many grades of Polyprop.. |
|||
CTE, linear | 132 µm/m-°C @Temperature -50.0 - 100 °C |
73.3 µin/in-°F @Temperature -58.0 - 212 °F |
|
Sorbothane Polyurethane Damping Material, 70 Durometer Sorbothane® is a thermoset, polyether-based polyurethane viscoelastic material that combines high energy absorption with faultless memory. Sorbothane turns mechanical energy into heat. As the mat.. |