Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 118 µm/m-°C @Temperature 20.0 °C |
65.6 µin/in-°F @Temperature 68.0 °F |
|
Cytec EN-2552 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |
|||
CTE, linear | 118 µm/m-°C @Temperature 20.0 °C |
65.6 µin/in-°F @Temperature 68.0 °F |
|
Cytec EN-2551 (Conap) Potting and Encapsulation Adhesive Polyurethane Potting and Encapsulating SystemsConathane® EN-2500 series polyurethane potting and encapsulating systems from Cytek have varying degrees of worklife, viscosity and hardness for many s.. |