Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9338 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9348 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | Y; IPC-TM-650.2.4.41 |
Park Electrochemical Nelco® NH9450 PTFE Laminate, Woven-Glass and Ceramic Reinforced The N9000 PTFE laminate system is designed for critical microwave components, antennas, power amplifiers and subassemblies. Superior mechanical and electrical performance make the N9000 PTFE laminat.. |
|||
CTE, linear | 12.0 - 500 µm/m-°C | 6.67 - 278 µin/in-°F | Average value: 104 µm/m-°C Grade Count:15 |
Overview of materials for Polyphthalamide (PPA), 50% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 50% Glass Fiber Reinforced". Each property range of values reported is minimum and maxi.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | Y-Direction; IPC-TM-650 2.4.41 |
Rogers Corporation RO3730 Antenna Grade Laminate RO3730™ Laminates have the excellent thermo-mechanical properties and electrical characteristics that antenna designers need. The laminates have a dielectric constant of 3.0 and a loss tangent of.. |
|||
CTE, linear | 12.0 - 55.0 µm/m-°C | 6.67 - 30.6 µin/in-°F | Average value: 20.4 µm/m-°C Grade Count:25 |
Overview of materials for Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Diallyl Phthalate (DAP) Molding Compound, Short Glass Fiber Filled". Each property range of values repor.. |
|||
CTE, linear | 12.0 - 50.0 µm/m-°C | 6.67 - 27.8 µin/in-°F | Average value: 28.7 µm/m-°C Grade Count:33 |
Overview of materials for Polycarbonate, 20% Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Polycarbonate, 20% Glass Filled". Specific grades with glass content between 15% and 24% are included. E.. |
|||
CTE, linear | 12.0 - 90.0 µm/m-°C | 6.67 - 50.0 µin/in-°F | Average value: 44.3 µm/m-°C Grade Count:14 |
Overview of materials for Epoxy, Cast, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Epoxy, Cast, Unreinforced". Each property range of values reported is minimum and maximum values of appr.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 °C |
6.67 µin/in-°F @Temperature 68.0 °F |
|
Cookson Group Plaskon® SMT-B-1F Epoxy Molding Compound for PBGAs
(discontinued **) Test specimens were transfer molded and post cured 4 hours at 175°C.An epoxy molding compound optimized specifically for PBGA applications. It has the same unique resin system as SMT-B-1, which mi.. |
|||
CTE, linear | 12.0 - 38.0 µm/m-°C | 6.67 - 21.1 µin/in-°F | Average value: 21.1 µm/m-°C Grade Count:36 |
Overview of materials for Phenolic, Novolac, Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Glass Filled". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 12.0 - 30.0 µm/m-°C | 6.67 - 16.7 µin/in-°F | Average value: 18.4 µm/m-°C Grade Count:14 |
Overview of materials for Phenolic, Novolac, Mineral/Glass Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Glass Filled". Each property range of values reported is minimum and maximum .. |
|||
CTE, linear | 12.0 - 57.6 µm/m-°C | 6.67 - 32.0 µin/in-°F | Average value: 18.2 µm/m-°C Grade Count:42 |
Overview of materials for Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled This property data is a summary of similar materials in the MatWeb database for the category "Polyphenylene Sulfide (PPS), Mineral/Glass-Fiber Filled". Each property range of values reported is mini.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 °C |
6.67 µin/in-°F @Temperature 68.0 °F |
|
Hoskins Manufacturing Alumel® Thermocouple Wire Type K - Std All values may vary dependent on specific design and usageAlumel® is a registered trade name of Hoskins Manufacturing.Capabilities: WireRibbonSquareInsulatedPlatedInformation provided by Californ.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | at Set Pt. |
Ferro CF 7567 Low-Temperature Sealing VITREOUS Typical Powder Form: TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet specific therm.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 0180 Unsaturated Polyester UP SMC 0180 is a general purpose SMC for applications in the field of electrical industry. Typical applications are housings, covers, wire distribution boxes and metering cabinets. The material meets t.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 0500 Unsaturated Polyester UP SMC 0500 is a special SMC with reduced density. The glass level has been selected to combine good moulding with good strength and stiffness properties. Even without a specific fire retardant the fir.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 0800 Unsaturated Polyester UP SMC 0800 is a special SMC for applications within househould and kitchenware. The glass level has been selected to combine good mouldability with good strength and stiffness properties. The product .. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 0900 Unsaturated Polyester UP SMC 0900 is a special SMC for use within a chemical aggressive environment. The glass level is selected to combine good mouldability with good strength and stiffness properties. The product is espec.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® SMC 1100 Unsaturated Polyester UP SMC 1100 is a special vinylester SMC for high strength applications. The reinforcement has been put to a level that combines mouldability with high strength and stiffness properties. The specific re.. |
|||
CTE, linear | 12.0 - 14.0 µm/m-°C @Temperature 20.0 °C |
6.67 - 7.78 µin/in-°F @Temperature 68.0 °F |
|
MMCC Al/Al2O3 Particulate Aluminum Matrix Composite Cast, discontinuously reinforced aluminum matrix composite. May be fabricated by vacuum infiltration of the ceramic preform.Data provided by the manufacturer, Metal Matrix Cast Composites (MMCC). |
|||
CTE, linear | 12.0 - 12.5 µm/m-°C @Temperature 20.0 - 150 °C |
6.67 - 6.94 µin/in-°F @Temperature 68.0 - 302 °F |
|
International Mold Steel Porcerax II Sintered, Porous Mold Steel Description: Porcerax II is a sintered, porous metal with porosity in the range of 20 to 30% by volume. A system of interconnected pores with an average diameter of 7 or 20 micron is dispersed throu.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | |
Mo-Sci Corporation GAI-40-I Green A Intruder Filter Glass Applications: Lead-free NVIS Green A Intruder filter glass for incandescent light sources.Information provided by Mo-Sci Corporation. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | ISO 11359-2 |
Menzolit Menzolit® BMC 2910 Unsaturated Polyester UP BMC 2910 incorporates additives which enhance the integral performance of mouldings during and after fire, currently used to mould Boltcaps which are designed to provide protection to the bolted co.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 100 °C |
6.67 µin/in-°F @Temperature 68.0 - 212 °F |
|
Special Metals NIMONIC® Alloy 115 A precipitation-hardenable nickel-chromium-cobalt alloy with an addition of molybdenum for solid-solution strengthening. It is similar to NIMONIC alloy 105 but has higher levels of aluminum and tit.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | |
Master Bond EP30LTE-LO Dimensionally Stable Low Outgassing Two Part Epoxy Master Bond Polymer System EP30LTE-LO is a thermal shock resistant epoxy resin system with low thermal expansion properties and dimensional stability for high performance bonding, sealing and castin.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 - 200 °C |
6.67 µin/in-°F @Temperature 68.0 - 392 °F |
Values determined by minute linear expansion tester at 5°C/min. temperature increments |
UBE UPILEX 25S (25 micron) Polyimide Film Description: UPILEX, the ultra-high heat-resistant polyimide film, is the product of the polycondensation reaction between biphenyltetracarboxylic dianhydride (BPDA), of which process Ube Industries.. |
|||
CTE, linear | 12.0 µm/m-°C @Temperature 20.0 °C |
6.67 µin/in-°F @Temperature 68.0 °F |
MD |
Toyobo TS201 PPS, Glass Fiber/Mineral Reinforced Key Feature: Standard high stiffness - used for metal replacementHigh performance injection-molding resin created from crystalline polyphenylene sulfide, using a special formulation technology devel.. |
|||
CTE, linear | 12.0 µm/m-°C | 6.67 µin/in-°F | |
Mo-Sci Corporation B-40-N Blue Filter Glass Applications: Lead-free NVIS blue filter glass for Nichia White LED sources.Information provided by Mo-Sci Corporation. |