Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 °C |
6.11 µin/in-°F @Temperature 68.0 °F |
TMA; ASTM E831 |
LNP Thermocomp® LC-1006 Polyetheretherketone, Carbon Fiber Reinforcement
(discontinued **) Forms: PelletsProcessing Method: Injection MoldingInformation provided by LNP, a GE Plastics Company.This data sheet is labeled Discontinued; however many LNP grades are still active under new names.. |
|||
CTE, linear | 11.0 - 237 µm/m-°C | 6.11 - 132 µin/in-°F | Average value: 74.8 µm/m-°C Grade Count:41 |
Overview of materials for Polytetrafluoroethylene (PTFE), Glass Filled, Molded This property data is a summary of similar materials in the MatWeb database for the category "Polytetrafluoroethylene (PTFE), Glass Filled, Molded". Each property range of values reported is minimum.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 465E2R30012 Natural, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 12%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 513E3720008 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 23%. Weight loss on heating = 1.2% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 335 µm/m-°C | 6.11 - 186 µin/in-°F | Average value: 133 µm/m-°C Grade Count:44 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |
|||
CTE, linear | 11.0 µm/m-°C | 6.11 µin/in-°F | DIN 53752 |
Lehmann & Voss LUVOCOM® 20-0951 Polyphthalamide, with carbon fiber Applications: Automotive industry, textile- and office machinery, apparatus- and precision engineering.High-strength and high-stiff parts; low coefficient of expansion.Electrically conductive, suita.. |
|||
CTE, linear | 11.0 µm/m-°C | 6.11 µin/in-°F | |
Mo-Sci Corporation GB-40-N Green B Filter Glass Applications: Lead-free NVIS Green B filter glass for white LED sources.Information provided by Mo-Sci Corporation. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 °C |
6.11 µin/in-°F @Temperature 68.0 °F |
|
Saint-Gobain Micaver® Glass-Mica Electrical Insulator, Transfer Moldings Glass-mica compound that occupies a place between plastics and ceramics in terms of usage temperature. It can be molded and machined like plastics and has the mechanical properties (strength, hardn.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 750 °C |
6.11 µin/in-°F @Temperature 68.0 - 1380 °F |
BSÂ 1902: section 5.3: 1990 |
Skamol Group V-1100 475 Vermiculite Insulating Slab SKAMOL V-1100 & VIP-12 vermiculite slabs have the following characteristics: Max. service temperature: Up to 1150°C (2102°F)Hot-face applications or back-up insulation of all refractory constr.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 - 750 °C |
6.11 µin/in-°F @Temperature 68.0 - 1380 °F |
BSÂ 1902: section 5.3: 1990 |
Skamol Group V-LITE 375 Vermiculite Insulating Brick V-LITE vermiculite insulating bricks have the following characteristics: Max. service temperature 1100°C (2012°F)Hot-face applications and back-up insulationGood insulation valueHigh mechanica.. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 °C |
6.11 µin/in-°F @Temperature 68.0 °F |
ASTM D 696 |
Lubrizol Isoplast® 101LGF60BLK Engineering Thermoplastic Polyurethane Resin Available in Americas, Europe, Middle East, Africa, India and AsiaData provided by LubrizolLubrizol acquired the Isoplast product line from Dow in 2009. |
|||
CTE, linear | 11.0 µm/m-°C @Temperature 20.0 °C |
6.11 µin/in-°F @Temperature 68.0 °F |
|
Goodfellow E-glass/Epoxy Composite Boro-silicate glass/EpoxyInformation provided by Goodfellow. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 285A2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 285A2R30023 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 16%. Weight loss on heating = 0.8% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 285A3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 485E2R30010 Natural, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 576E3720010 Clear, Trsp Cellulose Acetate Butyrate Plasticizer 10%. Weight loss on heating = 0.5% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 307A2R30018 Natural, Trsp Cellulose Acetate Propionate Plasticizer 18%. Weight loss on heating = 1% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pro.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 360E0096916 Natural, Trsp Cellulose Acetate Propionate Plasticizer 16%. Weight loss on heating = 1.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 377E4861312 Clear, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 380A4000010 Clear, Trsp Cellulose Acetate Propionate Plasticizer 10%. Weight loss on heating = 0.3% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 381E4000015 Clear, Trsp Cellulose Acetate Propionate Plasticizer 15%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Propionate 383A2R30012 Natural, Trsp Cellulose Acetate Propionate Plasticizer 12%. Weight loss on heating = 0.4% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of p.. |
|||
CTE, linear | 11.0 - 13.0 µm/m-°C @Temperature 1000 °C |
6.11 - 7.22 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories HRD-SNE Plate Brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 11.0 - 13.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 7.22 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance A-5 Alnico Magnetic Material |
|||
CTE, linear | 11.0 - 13.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 7.22 µin/in-°F @Temperature 68.0 °F |
Parallel DOM |
Alliance A-5DG Alnico Magnetic Material |
|||
CTE, linear | 11.0 - 170 µm/m-°C | 6.11 - 94.4 µin/in-°F | Average value: 44.8 µm/m-°C Grade Count:36 |
Overview of materials for Cellulose Acetate Butyrate, Molded This property data is a summary of similar materials in the MatWeb database for the category "Cellulose Acetate Butyrate, Molded". Each property range of values reported is minimum and maximum value.. |
|||
CTE, linear | 11.0 - 17.0 µm/m-°C @Temperature 20.0 °C |
6.11 - 9.44 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Eastman Tenite Butyrate 465E3720008 Clear, Trsp Cellulose Acetate Butyrate
(discontinued **) Plasticizer 8%. Weight loss on heating = 0.7% per ASTM D 707. Soluble matter loss = 0.1% per ASTM D 570.Product Description: TENITE cellulosic plastics are noted for their excellent balance of pr.. |