Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 72.0 µm/m-°C @Temperature -18.0 - 38.0 °C |
40.0 µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
Plaskolite Duraplex® 50% I Impact Modified Acrylic Sheet Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature -18.0 - 38.0 °C |
40.0 µin/in-°F @Temperature -0.400 - 100 °F |
ASTM D696 |
Plaskolite Duraplex® 70% I Impact Modified Acrylic Sheet Continuously processed acrylic sheet.Data provided by the manufacturer, Plaskolite, Inc. |
|||
CTE, linear | 72.0 - 79.2 µm/m-°C | 40.0 - 44.0 µin/in-°F | ASTM D696 |
Quantum Nylon 6/6 Information provided by Quantum Advanced Engineering Plastics |
|||
CTE, linear | 72.0 - 90.0 µm/m-°C @Temperature 0.000 - 156 °C |
40.0 - 50.0 µin/in-°F @Temperature 32.0 - 312 °F |
Average value: 76.5 µm/m-°C Grade Count:4 |
Overview of materials for Acrylic, Heat Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Heat Resistant, Molded". Each property range of values reported is minimum and maximum values o.. |
|||
CTE, linear | 72.0 - 162 µm/m-°C @Temperature 25.6 - 204 °C |
40.0 - 90.0 µin/in-°F @Temperature 78.0 - 400 °F |
ASTM D696 |
Technetics Group Texolon™ 7865 PTFE
(Unverified Data**) Virgin PTFE for those applications not requiring the premium qualities of 8764 sheet.PTFE CharacteristicsChemical ResistanceThermal StabilityCryogenic PropertiesLow Coefficient of FrictionLow Surfac.. |
|||
CTE, linear | 72.0 - 75.0 µm/m-°C | 40.0 - 41.7 µin/in-°F | Average value: 74.4 µm/m-°C Grade Count:5 |
Overview of materials for Styrene-Butadiene Copolymer, SBC This property data is a summary of similar materials in the MatWeb database for the category "Styrene-Butadiene Copolymer, SBC". Each property range of values reported is minimum and maximum values .. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech SP-3010 Rigid PVC Specialty Sheet Description: Specialty SheetInformation provided by Spartech. |
|||
CTE, linear | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D 696 |
Styrolution PS 1300/1301 GPPS Profile extrusionGood balance of flow and strengthHigh stiffnessUSP Class VI certifiedUL Classification 94 HBInformation provided by Styrolution |
|||
CTE, linear | 72.0 µm/m-°C | 40.0 µin/in-°F | ASTM D 696 |
Styrolution PS 1600 GPPS Foam extrusion; Injection moldingGood balanced of strength, flow and heat resistanceFree of zinc and oil additivesInformation provided by Styrolution |
|||
CTE, linear | 72.0 - 90.0 µm/m-°C @Temperature 20.0 °C |
40.0 - 50.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Ensinger Tecast Vekton™ 6PALM Premium Bearing Grade cast nylon (PA6) Tecast 6PALM contains both solid and liquid lubricants dispersed throughout the nylon to provide consistent wear rates and coefficients of friction.Information provided by Ensinger, Inc. |
|||
CTE, linear | 72.0 µm/m-°C | 40.0 µin/in-°F | T<Tg; 90 Minute UV Cure; SLA 3500 System; ASTM E831-93 |
3D Systems Accura® accuGen™ Nd Plastic for SLA® Systems Our most versatile material combines accuracy, green strength, and build chamber environment independence. For the SLA® Viper si2™, 3500, 5000 & 7000 systems.Typical ApplicationsMulti-purpose mode.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
|
Armstrong A-10-T Epoxy Adhesive Clear, thixotropic, 5-minute cure general-purpose epoxy adhesive. Provides rapid high strength bonds to many substrates. Supplied in 1:1 ratio dispense kits for easy application.Information provid.. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 7803 Rigid PVC, Extrusion High Impact Profile Information provided by Georgia GulfGeorgia Gulf became Axiall Corporation in 2013. |
|||
CTE, linear | 72.0 µm/m-°C @Temperature 20.0 °C |
40.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 6511 Rigid PVC, Molding Georgia Gulf 6511 is a special purpose rigid PVC compound designed for applications requiring the following properties: GlossImpact Strength & ToughnessFlame RetardantChemical ResistantThermoformab.. |
|||
CTE, linear | 72.0 - 100 µm/m-°C | 40.0 - 55.6 µin/in-°F | Average value: 88.4 µm/m-°C Grade Count:7 |
Overview of materials for Acrylic, Gamma Radiation Resistant, Molded This property data is a summary of similar materials in the MatWeb database for the category "Acrylic, Gamma Radiation Resistant, Molded". Each property range of values reported is minimum and maxim.. |