Thermal Properties Metric English Comments
CTE, linear 8.90 µm/m-°C
4.94 µin/in-°F
at Set Pt.
Ferro CF 7575 Display Device
Glass Type: Pb-Zn-B (Composite) Typical Powder Form: VSD Typical Application: Seal (Devitrified) Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for herm..
CTE, linear 8.90 µm/m-°C
4.94 µin/in-°F
at Set Pt. (Fired Thermal Expansion)
Ferro EG 2020 Low-Temperature Sealing
VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp..
CTE, linear 8.90 µm/m-°C

@Temperature 20.0 - 300 °C
4.94 µin/in-°F

@Temperature 68.0 - 572 °F
ISO 7991
Schott Glass 8516 Sealing Glass
Sealing glass for Fe-Ni alloys, high IR-absorbing, lead-free, of poor evaporation Reed switches The heavy metal content for the elements lead, cadmium, mercury, and hexavalent chromium is below 10..
CTE, linear 8.90 µm/m-°C

@Temperature 20.0 - 300 °C
4.94 µin/in-°F

@Temperature 68.0 - 572 °F
Schott S8008G Contrast Enhancement Filter
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.
CTE, linear 8.90 µm/m-°C

@Temperature 20.0 - 300 °C
4.94 µin/in-°F

@Temperature 68.0 - 572 °F
Schott S8807 Contrast Enhancement Filter
Contrast Enhancement FilterInformation Provided by SCHOTT North America, Inc.
CTE, linear 8.90 µm/m-°C

@Temperature 20.0 °C
4.94 µin/in-°F

@Temperature 68.0 °F
Sapco 99.7% Aluminum Oxide
Information provided by Sapco.
CTE, linear 8.90 µm/m-°C

@Temperature 20.0 °C
4.94 µin/in-°F

@Temperature 68.0 °F
Sapco 99.9% Aluminum Oxide
Information provided by Sapco.
CTE, linear 8.90 µm/m-°C

@Temperature 0.000 - 300 °C
4.94 µin/in-°F

@Temperature 32.0 - 572 °F
Corning 9010 Alkali Barium Crushed Glass
Used for sealing and other applications.Information provided by Corning Incorporated.
CTE, linear 8.90 µm/m-°C
4.94 µin/in-°F
at Set Pt. (Fired Thermal Expansion)
Ferro CF 7575 Low-Temperature Sealing
DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci..