Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.30 µm/m-°C | 4.61 µin/in-°F | |
Plansee W-20Cu Tungsten-Copper Composite This composite material is composed of a porous tungsten matrix which is infiltrated with copper.Characteristics:Very resistant to arc erosionGood electrical conductivityHigh thermal conductivityLow.. |
|||
CTE, linear | 8.30 µm/m-°C | 4.61 µin/in-°F | |
Poco Graphite PLS Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 260 °C |
4.61 µin/in-°F @Temperature 500 °F |
|
Ferro CF 7575 Display Device Glass Type: Pb-Zn-B (Composite) Typical Powder Form: VSD Typical Application: Seal (Devitrified) Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for herm.. |
|||
CTE, linear | 8.30 µm/m-°C | 4.61 µin/in-°F | at Set Pt. |
Ferro EG 2018 Display Device Glass Type: Pb-B (Composite) Typical Powder Form: VEG Typical Application: Seal Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and .. |
|||
CTE, linear | 8.30 µm/m-°C | 4.61 µin/in-°F | at Set Pt. |
Ferro EG 4020 Display Device Glass Type: Pb-B-AL Typical Powder Form: VSD Typical Application: Dielectric Ferro's display sealing glasses and dielectrics are low-temperature lead glasses suitable for hermetic sealing and pas.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 °C |
4.61 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech WCu20 Tungsten Copper Alloy Used to fabricate parts to near net size and several processes to produce high quality tungsten based materials.Tungsten heavy alloys have very high melting point and have a density twice that of st.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 25.0 - 600 °C |
4.61 µin/in-°F @Temperature 77.0 - 1110 °F |
|
ICE Steatite L-4 Data provided by the manufacturer, International Ceramic Engineering. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 °C |
4.61 µin/in-°F @Temperature 68.0 °F |
Parallel |
Momentive Performance Materials BNC2 Boron Nitride (BN) Refractory Composite Boron Nitride is a unique engineering material. It is a soft, machinable ceramic which can be combined with other refractory ceramics including Aluminum Oxide, Silicon Nitride, Aluminum Nitride, Mu.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 °C |
4.61 µin/in-°F @Temperature 68.0 °F |
|
TIMET TIMETAL® 679 (Ti-11Sn-5Zr-2.25Al-1Mo-0.2Si) Titanium Alloy; Quenched & Aged High-Temperature, High-Strength Creep Resistant AlloyIndustry Specifications: USA Aerospace: AMS 4974.Features: TIMETAL 679 has excellent tensile strength and is creep resistant up to 450°C. It i.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 - 200 °C |
4.61 µin/in-°F @Temperature 68.0 - 392 °F |
|
CeramTec 192/193 Titania 192/193 is an excellent material for textile and other structural applications, where superior surface finishes are required with high chemical resistance. 193 is identical except it is metallic gra.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 25.0 - 1000 °C |
4.61 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM-C372 |
CoorsTek DuraSense™ Ceramic Alumina Toughened Zirconia Oxygen ionic conductor for extreme-stress and extreme-thermal-shock environments |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 25.0 - 1000 °C |
4.61 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
CoorsTek Zirconia-Toughened Alumina, ZTA Thermal Shock Delta Tc = 300°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 - 1000 °C |
4.61 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Ceradyne Ceralloy® BeO Applications:collector rodshelix supportswindowsFeatures: higher thermal conductivity at room temperature.Information provided by Ceradyne Company |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 23.0 - 100 °C |
4.61 µin/in-°F @Temperature 73.4 - 212 °F |
|
ATI Wah Chang Vanadium Vanadium is widely dispersed in the earths crust occurring in many types of deposits. Most vanadium is currently obtained as a by-product or co product from titanomagnetites, petroleum, uranium ores.. |
|||
CTE, linear | 8.30 µm/m-°C | 4.61 µin/in-°F | |
Anderman Ceramics EAZ 20 Zirconia Toughened Alumina Zirconia materials offer high temperature capability as well as excellent performance in areas of high wear and corrosion. Available in many shapes and sizes. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 20.0 - 1000 °C |
4.61 µin/in-°F @Temperature 68.0 - 1830 °F |
|
CeramTec 950 Zirconia Toughened Alumina (ZTA), Al2O3•ZrO2 950 has a combination of high strength (from zirconia) and high hardness (from the alumina phase). It has excellent wear resistance, both in sliding and abrasive conditions. This material offers a g.. |
|||
CTE, linear | 8.30 µm/m-°C | 4.61 µin/in-°F | |
Poco Graphite Glassmate® SR Graphite An economical material for short production runs. An ideal insert material for thick bead transfer applications. |
|||
CTE, linear | 8.30 µm/m-°C @Temperature 260 °C |
4.61 µin/in-°F @Temperature 500 °F |
Fired Thermal Expansion |
Ferro CF 7575 Low-Temperature Sealing DEVITRIFYING Typical Powder Form: VSD, TF Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet speci.. |