Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 8.10 µm/m-°C | 4.50 µin/in-°F | |
Poco Graphite DFP Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
CTE, linear | 8.10 µm/m-°C | 4.50 µin/in-°F | |
Poco Graphite Glassmate® GM Graphite This material has high strength and durability for applications with high wear. An exceptional insert material for precision thread pick up and long production runs. |
|||
CTE, linear | 8.10 µm/m-°C | 4.50 µin/in-°F | |
Poco Graphite SFG Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
CTE, linear | 8.10 µm/m-°C | 4.50 µin/in-°F | |
Poco Graphite ZXF-5Q Industrial Grade Graphite SSH hardness is 86.General Poco Specialty Graphite Information: Poco's high strength, fine-grained, isotropic graphites offer maximum design flexibility. Easily machined. High strength and small p.. |
|||
CTE, linear | 8.10 µm/m-°C | 4.50 µin/in-°F | |
Poco Graphite DFP-3-2 Ion Implant Grade Graphite This is a high strength graphite that has reduced porosity. DFP-3-2 has long been the standard for components that exhibit long life and reduced erosion rates. |
|||
CTE, linear | 8.10 µm/m-°C | 4.50 µin/in-°F | |
Poco Graphite HPD Semiconductor Grade Graphite Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their .. |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 20.0 °C |
4.50 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials HCT-30 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 20.0 °C |
4.50 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials HCT-30D Titanium Diboride (TiB2) Powder Grade HCT-30D is tailored for fabrication by the hot-pressing process. Its composition provides for ease and optimizes the mechanical properties of the component shapes.Titanium Diboride Powder .. |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 20.0 °C |
4.50 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials HCT-40 Titanium Diboride (TiB2) Powder A high purity powder, grade HCT has virtually no second phase contaminants and only low, controlled levels of carbon, oxygen and nitrogen. Alkalis, alkaline earth, and most metals are typically u.. |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 20.0 °C |
4.50 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials HCT-F Titanium Diboride (TiB2) Powder Grade HCT-F powders are designed for use on applications requiring reduced particle size without sacrificing high purity.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced.. |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 20.0 °C |
4.50 µin/in-°F @Temperature 68.0 °F |
|
Momentive Performance Materials HCT-S Titanium Diboride (TiB2) Powder Grade HCT-S powder can be cold-pressed and sintered into high density (98% of theoretical), near-net shapes.Titanium Diboride Powder Titanium Diboride (TiB2) is produced by GE Advanced Ceramics usi.. |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 20.0 - 400 °C |
4.50 µin/in-°F @Temperature 68.0 - 752 °F |
DIN EN 821-1 |
CeramTec DC 25 Dispersion Ceramic, Al2O3-ZrO2 DC 25 is a ZTA Alumina Zirconia Platelet Composite used in dental applications. |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 25.0 - 1000 °C |
4.50 µin/in-°F @Temperature 77.0 - 1830 °F |
ASTM C372 |
CoorsTek AD-90 Alumina (nom. 90% Al2O3) Thermal Shock Delta Tc = 250°C - Thermal shock tests are performed by quenching samples in water from different elevated temperatures. Delta Tc is the change in temperature which results in a shar.. |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 20.0 °C |
4.50 µin/in-°F @Temperature 68.0 °F |
|
Cotronics Resbond™ 907 High Temperature Ceramic Adhesive, Industrial Strength |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 20.0 °C |
4.50 µin/in-°F @Temperature 68.0 °F |
|
Cotronics Resbond™ 908 High Temperature Ceramic Adhesive, Moisture Proof |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 20.0 °C |
4.50 µin/in-°F @Temperature 68.0 °F |
|
Cotronics Resbond™ 940 High Temperature Ceramic Adhesive, Fast Set |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 20.0 °C |
4.50 µin/in-°F @Temperature 68.0 °F |
|
Cotronics Resbond™ 989 High Temperature, High Purity Alumina Adhesive, General Purpose |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 25.0 - 1000 °C |
4.50 µin/in-°F @Temperature 77.0 - 1830 °F |
|
Astro Met ZTA 96 Zirconia Toughened Alumina General Description:ZTA-96 is a zirconia toughened alumina ceramic that exhibits excellent wear and corrosion resistance along with high strength and toughness. Astro Met has developed ZTA-96 zircon.. |
|||
CTE, linear | 8.10 µm/m-°C | 4.50 µin/in-°F | |
Aremco Ceramabond™ 685-N High Temperature Ceramic Adhesive/Paste, Zirconia Filled Aremco's ceramic adhesives are easy to use, one- and two-component systems which air dry in 1-2 hrs and are ready for use following a 200 to 700 °F cure. These materials are mostly water-based and.. |
|||
CTE, linear | 8.10 µm/m-°C | 4.50 µin/in-°F | |
Poco Graphite Glassmate® HT Graphite This high strength material has an oxidation inhibitor that raises the oxidation threshold. Service temperature can be raised to 600°C; graphites are subject to oxidation above 450°C |
|||
CTE, linear | 8.10 µm/m-°C @Temperature 20.0 °C |
4.50 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Edgetek® AM-30CF/000 Polyphthalamide (PPA), Carbon Fiber Reinforced
(discontinued **) Description/Features:Carbon Fiber ReinforcedPolyOne First ChoiceInformation provided by PolyOne Corporation. |