Thermal Properties Metric English Comments
CTE, linear 7.90 µm/m-°C
4.39 µin/in-°F
Poco Graphite AXF-5Q Industrial Grade Graphite
POCO’s specialty graphite materials are used in a wide range of highly technical and industrial applications. Each grade has characteristics and properties that allow the user to match the ideal gr..
CTE, linear 7.90 µm/m-°C
4.39 µin/in-°F
Poco Graphite TRA Semiconductor Grade Graphite
Although it is impossible to identify differences between various grades of graphite by looking at them, each grade has a special set of characteristics and physical properties that determine their ..
CTE, linear 7.90 - 121 µm/m-°C
4.39 - 67.2 µin/in-°F
Average value: 92.5 µm/m-°C Grade Count:43
Overview of materials for Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded
This property data is a summary of similar materials in the MatWeb database for the category "Acrylonitrile/Styrene/Acrylate (ASA), Unreinforced, Molded". Each property range of values reported is m..
CTE, linear 7.90 µm/m-°C
4.39 µin/in-°F
at Set Pt. (Fired Thermal Expansion)
Ferro EG 2012 Low-Temperature Sealing
VITREOUS, COMPOSITE Typical Powder Form: VEG Ferro's line of low-temperature sealing glasses are comprised of lead-borate (vitreous) and lead-zinc-borate crystallizing glasses formulated to meet sp..
CTE, linear 7.90 µm/m-°C

@Temperature 20.0 - 650 °C
4.39 µin/in-°F

@Temperature 68.0 - 1200 °F
Du-Co Ceramics DC-265-L-6 Alumina, 96% Al2O3
Properties reported below are averages from unglazed specimens. Tests performed to ASTM specifications. Actual values may vary. Information provided by DU-CO Ceramics Company.
CTE, linear 7.90 µm/m-°C
4.39 µin/in-°F
DIN EN 821-1
CeramTec 614/698 Alumina, 96%
614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink.
CTE, linear 7.90 µm/m-°C

@Temperature 27.0 °C
4.39 µin/in-°F

@Temperature 80.6 °F
Mateck Window Grade Zinc Selenide, ZnSe
Optical Crystals