Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : CTE, linear = 4.28 µin/in-°F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
CTE, linear 7.70 µm/m-°C
4.28 µin/in-°F
Poco Graphite AXF-5Q10W Biomedical Grade Graphite
POCO has developed post synthesis modifications to make our graphites more suitable to specific conditions. As a producer of highly technical, specialty materials, POCO also offers design engineerin..
CTE, linear 7.70 µm/m-°C

@Temperature 20.0 °C
4.28 µin/in-°F

@Temperature 68.0 °F
MarkeTech Aluminum Oxide Ceramic - Alumina 98%
Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture..
CTE, linear <= 7.70 µm/m-°C

@Temperature 20.0 °C
<= 4.28 µin/in-°F

@Temperature 68.0 °F
MarkeTech AO 95 Aluminum Oxide Ceramic Substrate, 95% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 4.0 x 6.0 in.. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 Â..
CTE, linear <= 7.70 µm/m-°C

@Temperature 20.0 °C
<= 4.28 µin/in-°F

@Temperature 68.0 °F
MarkeTech AO 98 Aluminum Oxide Ceramic Substrate, 98% Purity
Data provided by the supplier, MarkeTech International.Substrate Specs: Maximum dimensions 4.0 x 6.0 in.. Thickness 0.12-0.60 in. Surface roughness 0.3 µm as fired; 0.075 µm lapped; 0.025 Â..
CTE, linear 7.70 - 8.10 µm/m-°C

@Temperature 20.0 - 100 °C
4.28 - 4.50 µin/in-°F

@Temperature 68.0 - 212 °F
MarkeTech Cu/Mo/Cu 1:3:1 Laminated Sheet
Cu/MoCu sheets have very high in-plane thermal conductivity provide by layers of Cu and low CTEs provided by the inner layer of molybdenum. These laminated sheets spread heat from a concentrated hea..
CTE, linear 7.70 µm/m-°C

@Temperature 20.0 °C
4.28 µin/in-°F

@Temperature 68.0 °F
GBC Grade 98 Alumina
Data provided by the manufacturer, GBC Materials Corporation.
CTE, linear 7.70 µm/m-°C

@Temperature 260 °C
4.28 µin/in-°F

@Temperature 500 °F
Ferro EG 2992 Glaze and Sealant Glass
Glass Type: Bi-Zn-B Typical Powder Form: SRRG Typical Application: Ferrites Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insu..
CTE, linear 7.70 µm/m-°C

@Temperature 20.0 - 427 °C
4.28 µin/in-°F

@Temperature 68.0 - 801 °F
Special Metals INCOLOY® Alloy 907
A nickel-iron-cobalt alloy with additions of niobium and titanium for precipitation hardening. It has the low coefficient of expansion and high strength of INCOLOY alloy 903 but with improved notch..
CTE, linear 7.70 µm/m-°C

@Temperature 20.0 - 427 °C
4.28 µin/in-°F

@Temperature 68.0 - 801 °F
Special Metals INCOLOY® Alloy 909
A nickel-iron-cobalt alloy with a silicon addition and containing niobium and titanium for precipitation hardening. It is similar to INCOLOY alloys 903 and 907 in that it has low thermal expansion ..
CTE, linear 7.70 µm/m-°C
4.28 µin/in-°F
Accuratus Accuflect™ Light-Reflecting Ceramic
Accuflect™ is a specially formulated and processed ceramic developed by Accuratus to satisfy the market demand for diffuse reflectors in high temperature and high energy environments.Key Property: ..
CTE, linear 7.70 µm/m-°C

@Temperature 20.0 °C
4.28 µin/in-°F

@Temperature 68.0 °F
Aremco Ceramacast™ 575 Alumina Fine Grain Potting Compound
Hydraulic setting. Fine grain castable for potting and producing small tools. Used in the production of temperature probes, electrical feed-throughs, large heat treating fixtures, induction coils ..
CTE, linear 7.70 µm/m-°C

@Temperature 0.000 - 100 °C
4.28 µin/in-°F

@Temperature 32.0 - 212 °F
TIMET TIMETAL® 6-2-4-2 (Ti-6Al-2Sn-4Zr-2Mo-0.08Si) Titanium Alloy
Medium-Strength, Elevated Temperature AlloyIndustry Specifications: USA Aerospace: AMS 4919.Features: TIMETAL 6-2-4-2 has good tensile creep and fatigue properties up to 540°C. It is the most comm..
CTE, linear 7.70 µm/m-°C

@Temperature 20.0 - 600 °C
4.28 µin/in-°F

@Temperature 68.0 - 1110 °F
ASTM-C373
CeramTec 433 Alumina, 99.9%
433 (99.9%) is an alumina that exhibits high hardness. Its fine, equiaxial microstructure provides excellent sliding and abrasive wear resistance. This material is ideal for corrosive conditions. A ..
Copyright © lookpolymers.com All Rights Reserved