Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 7.50 µm/m-°C | 4.17 µin/in-°F | |
Plansee MoCu30 Molybdenum-Copper Characteristics:High thermal conductivityLow thermal expansionLow densityApplications:Electronic components - passive cooling elementsAutomotive industry - carrier plates for IGBT modules in electri.. |
|||
CTE, linear | 7.50 µm/m-°C | 4.17 µin/in-°F | |
Poco Graphite PYROGRAPH Ion Implant Grade Graphite Pyrograph is pyrolytically infiltrated graphite. POCO's proprietary process infiltrates the base material to a minimum depth of 0.1 inch throughout the entire surface of the component. This process .. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 °C |
4.17 µin/in-°F @Temperature 68.0 °F |
|
Zircar Zirconia Buster A-30 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
CTE, linear | 7.50 µm/m-°C | 4.17 µin/in-°F | at Set Pt. |
Ferro EG 2705 Glaze and Sealant Glass Glass Type: Ca-Al-Si Typical Powder Form: MVG Typical Application: Al2O3 Ferro's electronic and specialty glass group has produced over 3,000 formulations. Many are used as protective and insulat.. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 °C |
4.17 µin/in-°F @Temperature 68.0 °F |
|
MarkeTech Aluminum Oxide Ceramic - Alumina 96% Data provided by the supplier, MarkeTech International.Because of their high temperature, chemical, electrical, and mechanical properties along with their relatively low cost and ease of manufacture.. |
|||
CTE, linear | 7.50 µm/m-°C | 4.17 µin/in-°F | |
Mateck Al2O3 Substrate bicrystals for superconductivity |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 °C |
4.17 µin/in-°F @Temperature 68.0 °F |
|
GBC Grade 96 Alumina Data provided by the manufacturer, GBC Materials Corporation. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 °C |
4.17 µin/in-°F @Temperature 68.0 °F |
x-y direction |
MMCC Aluminum/Graphite Fiber GA 7-230 Metal Matrix Composite Discontinuous graphite fiber aluminum product primarily used for electronic thermal management applications. Lightweight, high damping, stiffer than aluminum, matched cte, easily machined and plate.. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 25.0 - 600 °C |
4.17 µin/in-°F @Temperature 77.0 - 1110 °F |
|
ICE Al2O3 94 Data provided by the manufacturer, International Ceramic Engineering. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 25.0 - 600 °C |
4.17 µin/in-°F @Temperature 77.0 - 1110 °F |
|
ICE Al2O3 96 Data provided by the manufacturer, International Ceramic Engineering. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.17 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Zircar Ceramics AL-30AAH Alumina Insulation AL-30AAH was developed for use in copper vapor lasers where the ultimate in low mass alumina purity is required.Information provided by Zircar Ceramics. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.17 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Zircar Ceramics ZAL-15AA Alumina Insulation ZAL-15 is a low thermal conductivity uniformly bound fiber board. It is ideal for machining into precision thermal insulators.Information provided by Zircar Ceramics. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 °C |
4.17 µin/in-°F @Temperature 68.0 °F |
|
Zircar Zirconia Buster A-30 Alumina Board, Disc, and Cylinder Insulation Zircar alumina insulation Type Buster is a rigid, fibrous ceramic material produced by vacuum forming alumina fibers with either a high purity alumina binder in BusterA-30 for use at 1600C or with s.. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 25.0 - 700 °C |
4.17 µin/in-°F @Temperature 77.0 - 1290 °F |
|
Du-Co Ceramics S-470 Aluminum Silicate Du-Co Ceramics Company manufactures a variety of crushable ceramic materials for use worldwide in cartridge heaters, thermocouples, and mineral insulated cable. The crushable ceramic products are cu.. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 1000 °C |
4.17 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SAL95 Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 1000 °C |
4.17 µin/in-°F @Temperature 1830 °F |
|
Chosun Refractories SAL99C Special High Alumina brick Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.17 µin/in-°F @Temperature 68.0 - 1830 °F |
|
BNZ Materials BNZP-23B Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.17 µin/in-°F @Temperature 68.0 - 1830 °F |
|
BNZ Materials BNZP-26 Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.17 µin/in-°F @Temperature 68.0 - 1830 °F |
|
BNZ Materials BNZP-26A Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.17 µin/in-°F @Temperature 68.0 - 1830 °F |
|
BNZ Materials BNZP-26HS Insulating Firebrick (French Grade) BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.17 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Anderman Ceramics EA96 Sintered Alumina, 96% High strength alumina (96%) available pink or white. Available in many shapes and sizes.Information provided by Anderman Ceramics. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.17 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Zircar Ceramics AL-30AA Alumina Insulation AL-30 and AL-30AA are rigid alumina fiber boards characterized by uniform open porosity and high machinability. Alumina bonded AL-30AA is used in fuel cell reformers.Information provided by Zircar C.. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.17 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Zircar Ceramics ALCAA Alumina Insulation ALC is the same material as ZAL-15 - but brings exceptional uniformity in an insulation material in cylindrical form.Information provided by Zircar Ceramics. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 1000 °C |
4.17 µin/in-°F @Temperature 68.0 - 1830 °F |
|
Zircar Ceramics ZAL-45AA Alumina Insulation ZAL-45 is an exceptionally strong low density alumina fiber product. Alumina bonded ZAL-45AA is useful in reducing conditions.Information provided by Zircar Ceramics. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 600 °C |
4.17 µin/in-°F @Temperature 68.0 - 1110 °F |
ASTM-C373 |
CeramTec 614/698 Alumina, 96% 614/698 (96%) is a high-strength alumina with good mechanical properties, as well as good wear and chemical resistance. It also features excellent electrical properties. 614 is white; 698 is pink. |
|||
CTE, linear | 7.50 µm/m-°C @Temperature 20.0 - 100 °C |
4.17 µin/in-°F @Temperature 68.0 - 212 °F |
DIN EN 821-1 |
CeramTec AT 79 Alumina, 99.6% Aluminas exhibit good mechanical properties such as hardness, compressive and tensile strength, and elastic modulus. They perform well at elevated temperatures. |