Thermal Properties | Metric | English | Comments |
---|---|---|---|
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
|
North Wood Plastics Polypropylene with 20% Wood Fiber, Molding Grade Data provided by North Wood Plastics, Inc. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
|
NOVA Chemicals Dylite® F271T Specialty Expandable Polystyrene Features: Highly consistent bead size; high gloss characteristics; low energy consumption; fast cyclingApplications: Drinking cups -hot and cold, noodle bowls, take-out and ice cream containers, and.. |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | |
NOVA Chemicals Dylite® F271TS Expandable Polystyrene Resin Highly consistent bead size, High gloss characteristics, Low energy consumption, Fast molding cycles, Food contact compliantApplications: Drinking cups (hot and cold), Noodle bowls, Take-out contai.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
|
North Wood Plastics Polypropylene with 20% Wood Fiber, Extrusion Grade Data provided by North Wood Plastics, Inc. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
PolyOne Lubri-Tech™ NL-15GM/15T Nylon 6/12, Glass Filled, PTFE Lubricated
(discontinued **) Description/Features:Milled Glass Fiber ReinforcedPTFE LubricatedUL 94 HBPolyOne First ChoiceInformation provided by PolyOne Corporation. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Spartech Royalite R6000 FR-PC Aircraft Grade Sheet Description: Aircraft Grade SheetInformation provided by Spartech. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature -46.0 - 93.0 °C |
35.0 µin/in-°F @Temperature -50.8 - 199 °F |
|
Sawbones Solid Rigid Polyurethane Foam 10 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature -46.0 - 93.0 °C |
35.0 µin/in-°F @Temperature -50.8 - 199 °F |
|
Sawbones Solid Rigid Polyurethane Foam 50 pcf Density Solid Rigid Polyurethane FoamPrimary UseSolid rigid polyurethane foam is primarily used as an alternative test medium for human cancellous bone. These products are not intended to replicate the mech.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 40.0 - 130 °C |
35.0 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 2408 Phenolic, Granular, Compression Molded PLENCO 02408 is a general purpose, organic filled phenolic molding compound, offering excellent cosmetic characteristics and improved electrical strength properties. UL recognized under component fi.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 40.0 - 130 °C |
35.0 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 2567 Phenolic, Granular, Compression Molded PLENCO 02567 is a general purpose, organic filled phenolic molding compound offering excellent cosmetic characteristics as typically required for vacuum metalized closures. UL recognized under compo.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Westlake Plastics Zelux® SD-P Polycarbonate (static dissipative) Carbon powder filled with high flexural strength and good thermal stability to 270°F. Thermoformable in 0.010" to 0.060" gauges; low outgassing.Information provided by Westlake Plastics. |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | Below Tg |
Tra-Con Tra-Bond 789-3 Moisture Resistant Adhesive TRA-BOND 789-3 one component, high strength toughened adhesive is designed for microelectronic applications, including substrate attach and package sealing, which require good moisture resistance. I.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
|
Tra-Con Tra-Bond F123HV Color Keyed Thixotropic Epoxy Adhesive TRA-BOND F123 HV is a fast cure, high viscosity, two-component epoxy formulation that signals both proper mixing and curing when bonding fiber optic bundles, potting glass fibers, and/or terminating.. |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | |
Trelleborg Emerson & Cuming EP574 Adhesive Clear unfilled adhesive for thin bond lines.All information provided by Trelleborg Emerson & Cuming |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | ASTM D696 |
Unitika M2350 PA6, Dry Nano composite nylonInformation provided by Unitika Ltd. |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | Below Tg |
Tra-Con Tra-Bond 789-3TN1 Moisture Resistant Adhesive TRA-BOND 789-3TN1 adhesive is a thixotropic version of TRA-BOND 789-3. It is a one component, high strength, toughened adhesive designed for use in applications which require good moisture resistanc.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
CPC - Vycom VINTEC® II TYPE II PVC Polyvinyl Chloride (PVC) Vintec II is a high impact, corrosion resistant polyvinyl chloride (PVC) sheet. Because of its excellent impact and ductility it is ideally suited for applications that require thermal forming or wh.. |
|||
CTE, linear | 63.0 µm/m-°C | 35.0 µin/in-°F | Below Tg |
Epoxy Technology EPO-TEK® MA-5 Optical Grade Epoxy Material Description: A single component, B-stageable, optical grade epoxy for fiber optic assembly. It may be used for B-stage sealing of fiber cables into ferrules, or fiber optic feed through in.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D-696 |
Axiall 3121 Rigid PVC, Extrusion Georgia Gulf 3121 is an exterior grade powder compound formulated for processing applications requiring high production output rate. Having excellent weatherability and impact strength, 3121 is sui.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Cast Nylons Nycast® Nyloil® Lubricated Nylon NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Cast Nylons Nycast® Nyloil®-MDX Lubricated Nylon, MoS2 Filled NYCAST® NYLOIL® was developed to extend the wear-resistant properties of unlubricated or dry lubricated materials such as MoS2 filled nylons. NYCAST® NYLOIL® will last 5 to 7 times longer than .. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 20.0 °C |
35.0 µin/in-°F @Temperature 68.0 °F |
ASTM D696 |
Asahi Kasei Thermofil P-9900-1760 Unreinforced, Heat Stabilized, Impact Modified Information provided by Asahi Thermofil |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 40.0 - 130 °C |
35.0 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 1581 Polyester, Briquette, Transfer Molded PLENCO 01581 is a glass and mineral reinforced pelletized polyester molding compound, exhibiting excellent dimensional stability, mechanical strength and also arc resistance, track resistance, and f.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature 40.0 - 130 °C |
35.0 µin/in-°F @Temperature 104 - 266 °F |
TMA; ASTM E831 |
Plenco 4311 Phenolic, Granular, Transfer Molded PLENCO 04311 is a heat resistant, mineral filled phenolic molding compound offering excellent processability, mechanical strength, and improved cold powder pourability characteristics. UL recognized.. |
|||
CTE, linear | 63.0 µm/m-°C @Temperature -30.0 - 100 °C |
35.0 µin/in-°F @Temperature -22.0 - 212 °F |
ASTM D696 |
LyondellBasell Hifax™ HSBMCB1158LS Thermoplastic Polyolefin Elastomer Description: Hifax™ HSBMCB1158LS high melt flow, 1,200 MPa flexural modulus, mineral filled thermoplastic elastomeric olefin (TEO) resin has a unique balance of flow, rigidity, low temperature impa.. |
|||
CTE, linear | 63.0 - 180 µm/m-°C | 35.0 - 100 µin/in-°F | Average value: 81.9 µm/m-°C Grade Count:62 |
Overview of materials for Nylon 6, Cast This property data is a summary of similar materials in the MatWeb database for the category "Nylon 6, Cast". Each property range of values reported is minimum and maximum values of appropriate MatW.. |
|||
CTE, linear | 63.0 - 310 µm/m-°C | 35.0 - 172 µin/in-°F | Average value: 214 µm/m-°C Grade Count:39 |
Overview of materials for Thermoset Polyurethane Foam, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Thermoset Polyurethane Foam, Unreinforced". Each property range of values reported is minimum and maximu.. |